Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.602 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 340.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 243.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 137.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 340.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 275.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 168.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 194.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 137.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 275.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 68.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 84.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 146.0 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 68.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 84.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 275.2 |
Al (mp-134) | <1 1 1> | <1 1 1> | 84.3 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 206.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 194.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 340.6 |
C (mp-66) | <1 1 0> | <1 1 1> | 252.8 |
C (mp-66) | <1 1 1> | <1 0 0> | 340.6 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 275.2 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 243.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 146.0 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 252.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 275.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 194.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 243.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 340.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 206.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 194.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 275.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 243.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 206.4 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 252.8 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 206.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 68.8 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 291.9 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 243.3 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 206.4 |
C (mp-66) | <1 0 0> | <1 1 1> | 252.8 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 168.5 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 243.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 146.0 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 206.4 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 206.4 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 252.8 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 243.3 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 206.4 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 252.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
76 | 88 | 88 | 0 | 0 | 0 |
88 | 76 | 88 | 0 | 0 | 0 |
88 | 88 | 76 | 0 | 0 | 0 |
0 | 0 | 0 | -52 | 0 | 0 |
0 | 0 | 0 | 0 | -52 | 0 |
0 | 0 | 0 | 0 | 0 | -52 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-53.1 | 28.5 | 28.5 | 0 | 0 | 0 |
28.5 | -53.1 | 28.5 | 0 | 0 | 0 |
28.5 | 28.5 | -53.1 | 0 | 0 | 0 |
0 | 0 | 0 | -19.4 | 0 | 0 |
0 | 0 | 0 | 0 | -19.4 | 0 |
0 | 0 | 0 | 0 | 0 | -19.4 |
Shear Modulus GV-33 GPa |
Bulk Modulus KV84 GPa |
Shear Modulus GR-13 GPa |
Bulk Modulus KR84 GPa |
Shear Modulus GVRH-23 GPa |
Bulk Modulus KVRH84 GPa |
Elastic Anisotropy7.87 |
Poisson's Ratio0.65 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd2AgIr (mp-977404) | 0.0000 | 0.048 | 3 |
PmNi2Sn (mp-862952) | 0.0000 | 0.000 | 3 |
TmZnPd2 (mp-865298) | 0.0000 | 0.011 | 3 |
Yb2AgGe (mp-865630) | 0.0000 | 0.000 | 3 |
LiTmPd2 (mp-867364) | 0.0000 | 0.015 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
ZnCo3 (mp-971744) | 0.0000 | 0.076 | 2 |
PbAu3 (mp-982246) | 0.0000 | 0.082 | 2 |
Ta3Ru (mp-977390) | 0.0000 | 0.000 | 2 |
Tl3Si (mp-972082) | 0.0000 | 0.344 | 2 |
V3Os (mp-866121) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pm_3 Zn Au |
Final Energy/Atom-3.7413 eV |
Corrected Energy-14.9653 eV
-14.9653 eV = -14.9653 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)