Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.388 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.104 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVPO5 + CsV3O8 + Cs2GaP3O10 + GaPO4 + O2 |
Band Gap0.658 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 0 -1> | 236.4 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 118.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 332.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 265.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 265.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 236.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 265.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 236.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 199.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 66.4 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 118.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 332.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 66.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 66.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 265.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 332.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 332.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 132.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 332.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 66.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 332.1 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 236.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 236.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 118.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 332.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 224.3 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 260.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 66.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 265.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 332.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 332.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 130.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 132.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 265.7 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 236.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 237.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 66.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 332.1 |
CdTe (mp-406) | <1 1 1> | <1 0 -1> | 236.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 332.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 332.1 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 199.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 332.1 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 132.8 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 -1> | 236.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 332.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 66.4 |
Mg (mp-153) | <0 0 1> | <1 0 -1> | 236.4 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 265.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 265.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
P3W2O13 (mp-767436) | 0.4412 | 0.011 | 3 |
P3W2O13 (mp-767085) | 0.4965 | 0.003 | 3 |
Mo2P3O13 (mp-504212) | 0.4534 | 0.009 | 3 |
Mo2P3O13 (mp-585184) | 0.4515 | 0.000 | 3 |
Mo2P3O13 (mp-704225) | 0.5082 | 0.000 | 3 |
LiP3W2O13 (mp-763480) | 0.5034 | 0.075 | 4 |
RbP2WO8 (mp-642422) | 0.4944 | 0.000 | 4 |
NaMo(PO4)2 (mp-622295) | 0.4847 | 0.012 | 4 |
RbP2WO8 (mp-560225) | 0.4921 | 0.000 | 4 |
RbMo2P3O13 (mp-19555) | 0.5129 | 0.000 | 4 |
V5O12 (mp-776915) | 0.6554 | 0.050 | 2 |
CsKMo4(P3O13)2 (mp-699557) | 0.3870 | 0.000 | 5 |
RbLiV(PO4)2 (mp-764302) | 0.7157 | 0.058 | 5 |
RbVGa(PO5)2 (mp-863294) | 0.2389 | 0.109 | 5 |
LiBS4(ClO3)4 (mp-555090) | 0.6199 | 0.005 | 5 |
LiV2S2(O4F3)2 (mp-769600) | 0.6711 | 0.051 | 5 |
RbScBP2HO9 (mp-23809) | 0.6739 | 0.000 | 6 |
CsAlBP2HO9 (mp-542129) | 0.5599 | 0.000 | 6 |
RbAlBP2HO9 (mp-542130) | 0.6268 | 0.000 | 6 |
KVBP2HO9 (mp-25623) | 0.6705 | 0.000 | 6 |
CsFeBP2HO9 (mp-761395) | 0.5747 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Cs_sv V_pv Ga_d P O |
Final Energy/Atom-6.6873 eV |
Corrected Energy-436.0595 eV
-436.0595 eV = -401.2399 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)