Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.489 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4P2O7 + Sn3(PO4)2 + LiPO3 |
Band Gap2.979 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 1 -1> | 260.3 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 260.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 138.0 |
GaP (mp-2490) | <1 1 1> | <0 1 -1> | 260.3 |
Si (mp-149) | <1 1 1> | <0 1 -1> | 260.3 |
Au (mp-81) | <1 0 0> | <0 1 -1> | 260.3 |
C (mp-48) | <1 0 1> | <0 1 -1> | 260.3 |
ZrO2 (mp-2858) | <1 1 0> | <1 1 -1> | 197.5 |
TiO2 (mp-390) | <1 0 0> | <0 1 -1> | 260.3 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 229.6 |
CaF2 (mp-2741) | <1 1 1> | <0 1 -1> | 260.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co3P4O15 (mp-850473) | 0.6621 | 0.170 | 3 |
Hg3SeO6 (mp-676169) | 0.6812 | 0.559 | 3 |
Cr3(AsO4)4 (mvc-6525) | 0.6606 | 0.225 | 3 |
Mn3(AsO4)4 (mvc-6676) | 0.6337 | 0.171 | 3 |
Sn3(AsO4)4 (mvc-6184) | 0.6484 | 0.182 | 3 |
LiFeP2O7 (mp-782726) | 0.4642 | 0.206 | 4 |
Li6Fe5(P2O7)4 (mp-705431) | 0.5231 | 0.278 | 4 |
Li14Mn9(P2O7)8 (mp-705402) | 0.4488 | 0.036 | 4 |
LiMnP2O7 (mp-695787) | 0.4643 | 0.098 | 4 |
Li2MnP2O7 (mp-705366) | 0.4982 | 0.363 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.6656 | 0.087 | 5 |
Li3MnV(P2O7)2 (mp-850951) | 0.6112 | 0.000 | 5 |
Li2V2SiGeO10 (mp-771932) | 0.6826 | 0.046 | 5 |
Li2SbP(OF3)2 (mp-776357) | 0.6486 | 0.088 | 5 |
Li3VCr(P2O7)2 (mp-765133) | 0.6288 | 0.018 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.5643 eV |
Corrected Energy-662.9342 eV
-662.9342 eV = -623.6060 eV (uncorrected energy) - 39.3282 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)