Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.539 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.055 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiSn2(PO3)5 + LiPO3 |
Band Gap3.798 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 234.0 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 190.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 146.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 273.3 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 117.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 234.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 146.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 273.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 117.0 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 190.2 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 234.0 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 234.0 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 234.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 234.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 273.3 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 146.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 273.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 117.0 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 273.3 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 146.4 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 190.2 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 273.3 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 234.0 |
C (mp-48) | <1 0 0> | <1 0 0> | 117.0 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 273.3 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 273.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 205.0 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 234.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 1> | 161.5 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 117.0 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 146.4 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 190.2 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 146.4 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 117.0 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 146.4 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 234.0 |
CaF2 (mp-2741) | <1 0 0> | <0 1 0> | 273.3 |
MgF2 (mp-1249) | <1 0 1> | <0 1 0> | 136.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaPO3 (mp-864891) | 0.5284 | 0.002 | 3 |
NaPO3 (mp-558192) | 0.5142 | 0.006 | 3 |
Hg2P2O7 (mp-28455) | 0.5446 | 0.000 | 3 |
Mn2P3O10 (mp-31981) | 0.4406 | 0.030 | 3 |
Cr2P3O10 (mp-31635) | 0.4774 | 0.057 | 3 |
LiSb2P5O16 (mp-684104) | 0.4346 | 0.048 | 4 |
LiBiP2O7 (mp-760637) | 0.4255 | 0.058 | 4 |
LiMn2(PO3)5 (mp-689938) | 0.4013 | 0.039 | 4 |
Li2Sn3(P2O7)2 (mp-757884) | 0.3837 | 0.073 | 4 |
Li2Ni(PO3)5 (mp-705005) | 0.4204 | 0.050 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.5159 | 0.087 | 5 |
MnFeCo(PO4)3 (mp-764410) | 0.6410 | 0.028 | 5 |
RbLiV(PO4)2 (mp-764302) | 0.6406 | 0.058 | 5 |
CaAl2Si4(H2O7)2 (mp-706640) | 0.5382 | 0.279 | 5 |
Li2Ti4Co(AsO5)4 (mp-744463) | 0.5830 | 0.010 | 5 |
LiMnVP2(HO5)2 (mp-765324) | 0.7460 | 0.041 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.7487 | 0.081 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.7723 eV |
Corrected Energy-274.2040 eV
-274.2040 eV = -257.3491 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|