Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.476 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 231.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 231.2 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 237.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 113.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 115.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 265.7 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 200.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 151.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 210.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 50.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 164.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 168.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 189.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 290.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 202.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 138.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 300.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 38.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 139.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 237.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 303.7 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 336.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 160.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 237.2 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 342.7 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 290.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 202.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 346.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 316.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 265.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 189.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 115.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 202.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 265.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 164.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 160.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 189.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 208.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 168.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 88.6 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 237.2 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 294.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 113.9 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 294.0 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 252.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 88.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 208.1 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 168.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 184.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgSnN2 (mp-1029791) | 0.2054 | 0.000 | 3 |
TiZnN2 (mp-1016108) | 0.2791 | 0.000 | 3 |
Mg2NbN3 (mp-1029408) | 0.2723 | 0.031 | 3 |
Mg2SbN3 (mp-1029378) | 0.1570 | 0.000 | 3 |
LiSn2N3 (mp-1029294) | 0.2716 | 0.070 | 3 |
Li4Fe3CoO8 (mp-771610) | 0.2588 | 0.075 | 4 |
LiCo7O7F (mp-764039) | 0.2197 | 0.061 | 4 |
Li4FeCo3O8 (mp-773339) | 0.2928 | 0.120 | 4 |
LiCo5O5F (mp-764225) | 0.2329 | 0.069 | 4 |
Li5CoOF5 (mp-853165) | 0.2633 | 0.037 | 4 |
PrH (mp-975657) | 0.1483 | 0.082 | 2 |
MnO (mp-999539) | 0.0948 | 0.005 | 2 |
TbSe (mp-10645) | 0.0959 | 0.525 | 2 |
CdO (mp-13119) | 0.0846 | 0.007 | 2 |
ZrN (mp-13126) | 0.0854 | 0.448 | 2 |
Ge (mp-1007760) | 0.3558 | 0.022 | 1 |
Si (mp-165) | 0.3613 | 0.013 | 1 |
C (mp-611426) | 0.4934 | 0.146 | 1 |
C (mp-47) | 0.3655 | 0.162 | 1 |
Ge (mp-1091415) | 0.4925 | 0.014 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pm_3 H |
Final Energy/Atom-4.4710 eV |
Corrected Energy-17.8838 eV
-17.8838 eV = -17.8838 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)