Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.340 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 273.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 284.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 164.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 309.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 309.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 154.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 232.0 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 232.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 273.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 232.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 232.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 284.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 284.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 154.7 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 328.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 273.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 273.4 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 154.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 218.7 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 232.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 54.7 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 232.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 218.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 328.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 218.7 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 232.0 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 284.2 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 284.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 273.4 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 273.4 |
BN (mp-984) | <0 0 1> | <1 1 1> | 284.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 94.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 273.4 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 309.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 273.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 284.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 273.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 273.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 273.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 232.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 218.7 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 164.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 328.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 94.7 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 1> | 284.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 273.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 154.7 |
C (mp-66) | <1 0 0> | <1 1 1> | 189.4 |
C (mp-66) | <1 1 0> | <1 1 0> | 309.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 273.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
81 | 54 | 54 | 0 | 0 | 0 |
54 | 81 | 54 | 0 | 0 | 0 |
54 | 54 | 81 | 0 | 0 | 0 |
0 | 0 | 0 | 31 | 0 | 0 |
0 | 0 | 0 | 0 | 31 | 0 |
0 | 0 | 0 | 0 | 0 | 31 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
26.5 | -10.6 | -10.6 | 0 | 0 | 0 |
-10.6 | 26.5 | -10.6 | 0 | 0 | 0 |
-10.6 | -10.6 | 26.5 | 0 | 0 | 0 |
0 | 0 | 0 | 32.3 | 0 | 0 |
0 | 0 | 0 | 0 | 32.3 | 0 |
0 | 0 | 0 | 0 | 0 | 32.3 |
Shear Modulus GV24 GPa |
Bulk Modulus KV63 GPa |
Shear Modulus GR20 GPa |
Bulk Modulus KR63 GPa |
Shear Modulus GVRH22 GPa |
Bulk Modulus KVRH63 GPa |
Elastic Anisotropy0.87 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm2MgRu (mp-972493) | 0.0000 | 0.099 | 3 |
Y2CuIr (mp-865594) | 0.0000 | 0.015 | 3 |
PaTlAu2 (mp-862830) | 0.0000 | 0.000 | 3 |
PmGaAu2 (mp-862905) | 0.0000 | 0.001 | 3 |
YbInHg2 (mp-865790) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
K3Hg (mp-983388) | 0.0000 | 0.063 | 2 |
SbPt3 (mp-973353) | 0.0000 | 0.123 | 2 |
ScZn3 (mp-973143) | 0.0000 | 0.018 | 2 |
ReSn3 (mp-974545) | 0.0000 | 0.743 | 2 |
PmH3 (mp-862910) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 Tl_d Ag |
Final Energy/Atom-3.9231 eV |
Corrected Energy-15.6924 eV
-15.6924 eV = -15.6924 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)