Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.535 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVP2O7 + LiPO3 + VPO5 + O2 |
Band Gap1.012 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 247.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 165.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 139.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 139.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 139.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 139.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 139.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 139.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 82.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 247.7 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 139.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 247.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 139.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 82.6 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 165.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 139.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 165.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 247.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 247.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 247.7 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 165.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 139.7 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 165.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 247.7 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 139.7 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 139.7 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 165.1 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 165.1 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 139.7 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 1> | 162.5 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 247.7 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 139.7 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 165.1 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 139.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn7Cr12O48 (mp-774029) | 0.4835 | 0.078 | 3 |
Cr(PO3)3 (mp-31690) | 0.5366 | 0.093 | 3 |
Ti7Cr12O48 (mp-853216) | 0.4496 | 0.084 | 3 |
Fe2(MoO4)3 (mvc-8023) | 0.5372 | 0.047 | 3 |
Cr(PO3)3 (mp-694576) | 0.5351 | 0.093 | 3 |
Li3V3P8O29 (mp-764116) | 0.1416 | 0.048 | 4 |
Li3V3P8O29 (mp-764077) | 0.1170 | 0.049 | 4 |
Li3V3P8O29 (mp-863891) | 0.1436 | 0.046 | 4 |
Li3V3P8O29 (mp-765983) | 0.1376 | 0.052 | 4 |
Li3V3P8O29 (mp-761830) | 0.1357 | 0.053 | 4 |
Cr19O48 (mp-850874) | 0.4530 | 0.097 | 2 |
Cr19O48 (mp-780521) | 0.4755 | 0.085 | 2 |
Mg7VFeMo15O56 (mp-743786) | 0.6863 | 0.011 | 5 |
MgVFeMo3O14 (mp-705896) | 0.6819 | 0.020 | 5 |
LiSn2P4H3O16 (mp-754500) | 0.5855 | 0.059 | 5 |
SnP4H8N2O13 (mp-603633) | 0.5203 | 0.010 | 5 |
TiP4H8N2O13 (mp-603612) | 0.6416 | 0.026 | 5 |
Ti2P4H9C2NO16 (mp-709069) | 0.5822 | 0.039 | 6 |
FeBP2H5NO9 (mp-766957) | 0.6800 | 0.005 | 6 |
VBP2H5NO9 (mp-25798) | 0.6353 | 0.000 | 6 |
AlBP2H5NO9 (mp-24757) | 0.7057 | 0.000 | 6 |
NaMgAl3Si8(HO6)4 (mp-1094103) | 0.5894 | 0.027 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.6660 | 0.050 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.0546 eV |
Corrected Energy-657.5245 eV
-657.5245 eV = -606.6997 eV (uncorrected energy) - 40.7328 eV (MP Anion Correction) - 10.0920 eV (MP Advanced Correction)
|