Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.798 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2SiO4 + Li2Si2O5 + Li2SiO3 |
Band Gap1.644 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmn21 [31] |
HallP 2ac 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 295.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 216.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 221.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 144.5 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 295.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 216.8 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 221.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 144.5 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 295.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 204.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 216.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 125.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 221.7 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 250.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 102.3 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 206.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 125.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 216.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 206.7 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 221.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 216.8 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 221.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 72.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 144.5 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 103.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 72.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 221.7 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 216.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 289.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 216.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 216.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 204.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 216.8 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 295.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 289.1 |
MgO (mp-1265) | <1 1 1> | <1 1 0> | 126.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 206.7 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 252.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 102.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 72.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 295.6 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 216.8 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 289.1 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 252.5 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 0 1> | 216.8 |
LaF3 (mp-905) | <1 0 0> | <0 1 1> | 103.4 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 147.8 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 147.8 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 295.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 73.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr5(PO4)4 (mp-540446) | 0.6210 | 0.007 | 3 |
Ca12Al14O33 (mp-530149) | 0.6879 | 0.007 | 3 |
Sr10Ga6O19 (mp-680384) | 0.7142 | 0.013 | 3 |
Ca3(AlN2)2 (mp-29820) | 0.7253 | 0.000 | 3 |
Cr5(PO4)4 (mp-775246) | 0.6281 | 0.007 | 3 |
Li2Fe(SiO3)2 (mp-863888) | 0.2211 | 0.273 | 4 |
Li4Ni2(PO4)3 (mp-853237) | 0.5229 | 0.116 | 4 |
Li2Si2NiO6 (mp-766931) | 0.2490 | 0.117 | 4 |
Li2Mn(SiO3)2 (mp-761485) | 0.1314 | 0.072 | 4 |
Li3Sc2(PO4)3 (mp-6565) | 0.4938 | 0.000 | 4 |
Li6VSn3(PO4)6 (mp-775752) | 0.4975 | 0.080 | 5 |
Li6Cr3Sb(PO4)6 (mp-762153) | 0.5279 | 0.058 | 5 |
Li6CrSn3(PO4)6 (mp-771364) | 0.4519 | 0.118 | 5 |
Li6MnSn3(PO4)6 (mp-771360) | 0.4425 | 0.065 | 5 |
Li3MnV(PO4)3 (mp-779098) | 0.5227 | 0.325 | 5 |
Li4TiFe3Cu2(PO4)6 (mp-778677) | 0.5865 | 0.081 | 6 |
Li4Mn2NbNi3(PO4)6 (mp-776611) | 0.5837 | 0.101 | 6 |
Li4Fe2Ni3Sn(PO4)6 (mp-781476) | 0.5890 | 0.081 | 6 |
Li4V3Cr2Co(PO4)6 (mp-771298) | 0.6030 | 0.122 | 6 |
Li4TiCu2Ni3(PO4)6 (mp-776613) | 0.5379 | 0.101 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Si O |
Final Energy/Atom-7.1207 eV |
Corrected Energy-505.3381 eV
-505.3381 eV = -469.9636 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 10.0920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)