Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.253 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 99.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 287.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 299.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 244.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 57.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 81.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 287.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 162.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 172.7 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 299.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 244.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 287.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 162.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 244.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 299.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 244.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 172.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 162.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 287.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 287.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 287.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 199.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 162.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 244.2 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 299.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 162.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 230.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 172.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 57.6 |
BN (mp-984) | <1 1 0> | <1 1 0> | 162.8 |
BN (mp-984) | <1 1 1> | <1 0 0> | 230.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 287.8 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 299.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 287.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 172.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 244.2 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 230.2 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 244.2 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 299.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 287.8 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 99.7 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 230.2 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 230.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 287.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 1> | 299.1 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 287.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 230.2 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 287.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 287.8 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 115.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
67 | 40 | 40 | 0 | 0 | 0 |
40 | 67 | 40 | 0 | 0 | 0 |
40 | 40 | 67 | 0 | 0 | 0 |
0 | 0 | 0 | 43 | 0 | 0 |
0 | 0 | 0 | 0 | 43 | 0 |
0 | 0 | 0 | 0 | 0 | 43 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
27.5 | -10.3 | -10.3 | 0 | 0 | 0 |
-10.3 | 27.5 | -10.3 | 0 | 0 | 0 |
-10.3 | -10.3 | 27.5 | 0 | 0 | 0 |
0 | 0 | 0 | 23.2 | 0 | 0 |
0 | 0 | 0 | 0 | 23.2 | 0 |
0 | 0 | 0 | 0 | 0 | 23.2 |
Shear Modulus GV31 GPa |
Bulk Modulus KV49 GPa |
Shear Modulus GR23 GPa |
Bulk Modulus KR49 GPa |
Shear Modulus GVRH27 GPa |
Bulk Modulus KVRH49 GPa |
Elastic Anisotropy1.87 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YHoCd2 (mp-979429) | 0.0000 | 0.006 | 3 |
Sm2AgSn (mp-972511) | 0.0000 | 0.025 | 3 |
Mn2CrCo (mp-864955) | 0.0000 | 0.000 | 3 |
LiNd2Ga (mp-865578) | 0.0000 | 0.004 | 3 |
LiLa2Os (mp-867813) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
K3Hg (mp-983388) | 0.0000 | 0.063 | 2 |
Yb3Os (mp-980006) | 0.0000 | 0.236 | 2 |
SmAg3 (mp-862736) | 0.0000 | 0.034 | 2 |
SmCd3 (mp-867158) | 0.0000 | 0.000 | 2 |
Rb3Ho (mp-974962) | 0.0000 | 0.641 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Mg_pv Al |
Final Energy/Atom-3.9735 eV |
Corrected Energy-15.8941 eV
-15.8941 eV = -15.8941 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)