Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.147 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 168.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 277.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 279.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 158.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 168.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 158.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 39.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 56.0 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 68.6 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 168.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 158.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 197.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 335.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 335.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 316.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 39.6 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 68.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 158.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 316.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 274.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 197.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 197.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 356.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 197.9 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 205.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 316.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 335.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 277.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 39.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 56.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 68.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 56.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 79.2 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 205.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 112.0 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 197.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 223.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 197.9 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 274.3 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 274.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 197.9 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 197.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 158.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 223.9 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 205.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 68.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 197.9 |
BN (mp-984) | <1 0 1> | <1 1 0> | 335.9 |
BN (mp-984) | <1 1 0> | <1 1 1> | 68.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 277.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
131 | 122 | 122 | 0 | 0 | 0 |
122 | 131 | 122 | 0 | 0 | 0 |
122 | 122 | 131 | 0 | 0 | 0 |
0 | 0 | 0 | 58 | 0 | 0 |
0 | 0 | 0 | 0 | 58 | 0 |
0 | 0 | 0 | 0 | 0 | 58 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
74.1 | -35.7 | -35.7 | 0 | 0 | 0 |
-35.7 | 74.1 | -35.7 | 0 | 0 | 0 |
-35.7 | -35.7 | 74.1 | 0 | 0 | 0 |
0 | 0 | 0 | 17.1 | 0 | 0 |
0 | 0 | 0 | 0 | 17.1 | 0 |
0 | 0 | 0 | 0 | 0 | 17.1 |
Shear Modulus GV37 GPa |
Bulk Modulus KV125 GPa |
Shear Modulus GR10 GPa |
Bulk Modulus KR125 GPa |
Shear Modulus GVRH24 GPa |
Bulk Modulus KVRH125 GPa |
Elastic Anisotropy13.08 |
Poisson's Ratio0.41 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrAlRu2 (mp-977436) | 0.0000 | 0.000 | 3 |
Sr2SbAu (mp-863251) | 0.0000 | 0.000 | 3 |
LiY2Rh (mp-862672) | 0.0000 | 0.010 | 3 |
Sr2CdPb (mp-862721) | 0.0000 | 0.000 | 3 |
Tm2OsPd (mp-865374) | 0.0000 | 0.000 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.007 | 4 |
VGaFeCo (mp-1066581) | 0.0000 | 0.029 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
Yb3V (mp-979942) | 0.0000 | 0.458 | 2 |
Si3Se (mp-978501) | 0.0000 | 0.785 | 2 |
Li3Mg (mp-976256) | 0.0000 | 0.006 | 2 |
ScTc3 (mp-867262) | 0.0000 | 0.000 | 2 |
Rb3Dy (mp-975013) | 0.0000 | 0.642 | 2 |
Xe (mp-979285) | 0.0000 | 0.002 | 1 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Cu_pv Au |
Final Energy/Atom-3.1233 eV |
Corrected Energy-12.4930 eV
-12.4930 eV = -12.4930 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)