Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.427 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 1> | 248.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 335.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 135.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 287.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 191.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 239.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 239.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 270.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 203.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 270.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 270.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 165.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 191.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 135.5 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 287.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 67.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 83.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 143.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 203.2 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 143.7 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 248.9 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 270.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 239.5 |
Al (mp-134) | <1 1 1> | <1 1 1> | 83.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 335.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 239.5 |
Al (mp-134) | <1 1 0> | <1 1 0> | 67.7 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 203.2 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 287.4 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 203.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 239.5 |
C (mp-66) | <1 1 0> | <1 1 0> | 203.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 1> | 165.9 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 165.9 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 191.6 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 239.5 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 239.5 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 248.9 |
GaP (mp-2490) | <1 1 1> | <1 1 0> | 270.9 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 239.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 335.3 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 270.9 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 239.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 143.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 203.2 |
Ni (mp-23) | <1 0 0> | <1 1 1> | 248.9 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 335.3 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 203.2 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 239.5 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 135.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlVFeCo (mp-1008530) | 0.0000 | 0.028 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.198 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.025 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.009 | 4 |
ZrPd (mp-13496) | 0.0000 | 0.066 | 2 |
SrCd (mp-30496) | 0.0000 | 0.000 | 2 |
Yb3In (mp-980052) | 0.0000 | 0.062 | 2 |
SiRh (mp-10110) | 0.0000 | 0.281 | 2 |
LuRh (mp-377) | 0.0000 | 0.000 | 2 |
NdCdPd2 (mp-977557) | 0.0000 | 0.000 | 3 |
Ti2ReTc (mp-972241) | 0.0000 | 0.013 | 3 |
SrHf2Mo (mp-631313) | 0.0000 | 0.934 | 3 |
BeGe2Te (mp-631450) | 0.0000 | 0.799 | 3 |
AcMgHg2 (mp-866225) | 0.0000 | 0.000 | 3 |
Ge (mp-998883) | 0.0000 | 0.346 | 1 |
Ni (mp-1008728) | 0.0000 | 0.097 | 1 |
Si (mp-1014212) | 0.0000 | 0.541 | 1 |
Cu (mp-998890) | 0.0000 | 0.034 | 1 |
Al (mp-998860) | 0.0000 | 0.095 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points28 |
U Values-- |
PseudopotentialsVASP PAW: Pa Al Au |
Final Energy/Atom-5.3755 eV |
Corrected Energy-21.5022 eV
-21.5022 eV = -21.5022 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)