material

TiFeSi

ID:

mp-8648

DOI:

10.17188/1310163


Tags: Titanium iron silicide (1/1/1) Iron titanium silicide (1/1/1)

Material Details

Final Magnetic Moment
0.158 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.735 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.62 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Ima2 [46]
Hall
I 2 2a
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 41157 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 0 0> <0 1 0> 0.008 269.1
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.037 223.8
GaTe (mp-542812) <1 0 0> <0 1 0> 0.075 134.5
AlN (mp-661) <0 0 1> <0 1 0> 0.095 67.3
ZrO2 (mp-2858) <1 1 0> <0 1 0> 0.097 201.8
LaAlO3 (mp-2920) <0 0 1> <1 1 0> 0.098 100.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.108 217.2
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.116 304.1
SiC (mp-11714) <1 0 1> <0 0 1> 0.118 130.3
CdSe (mp-2691) <1 1 0> <0 0 1> 0.133 217.2
Al (mp-134) <1 1 0> <0 0 1> 0.136 347.6
AlN (mp-661) <1 0 0> <0 0 1> 0.150 217.2
GaSb (mp-1156) <1 1 0> <0 0 1> 0.152 217.2
SiC (mp-8062) <1 1 1> <0 1 0> 0.154 67.3
MgO (mp-1265) <1 1 0> <1 0 1> 0.173 259.0
Te2W (mp-22693) <0 1 0> <0 0 1> 0.174 217.2
ZnTe (mp-2176) <1 0 0> <0 1 0> 0.174 269.1
InAs (mp-20305) <1 0 0> <0 1 0> 0.182 269.1
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.184 347.6
PbSe (mp-2201) <1 1 0> <0 0 1> 0.186 217.2
LaF3 (mp-905) <0 0 1> <0 1 0> 0.210 134.5
AlN (mp-661) <1 0 1> <0 0 1> 0.219 217.2
Mg (mp-153) <1 1 1> <0 1 0> 0.238 269.1
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.270 217.2
CdS (mp-672) <1 0 0> <1 0 1> 0.275 86.3
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.278 217.2
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.280 217.2
AlN (mp-661) <1 1 1> <1 0 0> 0.281 223.8
CdWO4 (mp-19387) <1 1 1> <0 0 1> 0.284 260.7
NaCl (mp-22862) <1 0 0> <0 1 1> 0.309 160.2
CdS (mp-672) <1 0 1> <1 0 0> 0.311 298.4
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.312 134.5
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.315 347.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.321 304.1
SiC (mp-11714) <1 1 1> <1 0 0> 0.323 223.8
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.342 304.1
CdS (mp-672) <1 1 0> <1 0 0> 0.348 149.2
SiO2 (mp-6930) <1 0 1> <1 0 1> 0.351 172.6
YVO4 (mp-19133) <1 1 0> <0 0 1> 0.356 130.3
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.361 223.8
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.366 223.8
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.377 259.0
Te2W (mp-22693) <0 0 1> <0 0 1> 0.385 43.4
BaF2 (mp-1029) <1 0 0> <0 1 1> 0.407 80.1
C (mp-48) <1 1 1> <1 0 0> 0.429 298.4
Y3Fe5O12 (mp-19648) <1 0 0> <0 1 1> 0.434 160.2
Ni (mp-23) <1 0 0> <1 0 0> 0.455 74.6
GaN (mp-804) <1 0 1> <0 1 0> 0.456 134.5
Te2W (mp-22693) <1 0 1> <0 1 0> 0.462 201.8
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.468 347.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
264 131 144 0 0 0
131 332 99 0 0 0
144 99 306 0 0 0
0 0 0 113 0 0
0 0 0 0 137 0
0 0 0 0 0 139
Compliance Tensor Sij (10-12Pa-1)
5.8 -1.6 -2.2 0 0 0
-1.6 3.8 -0.5 0 0 0
-2.2 -0.5 4.5 0 0 0
0 0 0 8.9 0 0
0 0 0 0 7.3 0
0 0 0 0 0 7.2
Shear Modulus GV
113 GPa
Bulk Modulus KV
183 GPa
Shear Modulus GR
105 GPa
Bulk Modulus KR
183 GPa
Shear Modulus GVRH
109 GPa
Bulk Modulus KVRH
183 GPa
Elastic Anisotropy
0.40
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZrGeRu (mp-637736) 0.2032 0.000 3
MnGeRh (mp-18649) 0.3440 0.000 3
PrZnRh (mp-607715) 0.5301 0.000 3
LaZnRh (mp-570525) 0.5558 0.000 3
TiSiRu (mp-11560) 0.1707 0.000 3
Mg3Al9FeSi5 (mp-7062) 0.6589 0.008 4
K2BaCdSb2 (mp-863761) 0.6940 0.000 4
K2SrCdSb2 (mp-863758) 0.7000 0.000 4
Mg3Al8FeSi6 (mp-571315) 0.6939 0.141 4
U3Al3NiRu2 (mp-1080528) 0.6886 0.097 4
USe2 (mp-8591) 0.6106 0.028 2
Ti2P (mp-30218) 0.6238 0.000 2
CeSe2 (mp-1021484) 0.6282 0.043 2
Mg4Si3 (mp-1074320) 0.6333 0.165 2
US2 (mp-2849) 0.6148 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Fe_pv Si
Final Energy/Atom
-7.9958 eV
Corrected Energy
-143.9252 eV
-143.9252 eV = -143.9252 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 41157
  • 633588
Submitted by
User remarks:
  • Titanium iron silicide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)