Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.650 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaPO3 |
Band Gap5.137 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 254.8 |
C (mp-48) | <1 0 0> | <0 0 1> | 152.9 |
C (mp-48) | <1 0 1> | <0 1 0> | 333.8 |
C (mp-48) | <1 1 0> | <0 1 0> | 166.9 |
C (mp-48) | <1 1 1> | <1 0 0> | 173.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 278.2 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 278.2 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 217.9 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 270.3 |
AlN (mp-661) | <1 1 0> | <1 -1 -1> | 267.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 254.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 254.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 278.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 203.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 234.5 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 1> | 297.7 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 0> | 238.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 156.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.9 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 234.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 243.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 166.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 -1> | 267.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 278.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 254.8 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 257.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 254.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 278.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 254.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 278.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 254.8 |
InP (mp-20351) | <1 1 0> | <1 -1 1> | 99.2 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 305.8 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 290.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 -1> | 257.8 |
CdWO4 (mp-19387) | <0 0 1> | <1 -1 0> | 238.0 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 288.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 278.2 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 254.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 0> | 166.9 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 0> | 162.1 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 234.5 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 0> | 317.4 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 234.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 254.8 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 202.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 152.9 |
BN (mp-984) | <1 0 1> | <1 -1 -1> | 178.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 278.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 152.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaV(SiO3)2 (mvc-6891) | 0.4457 | 0.169 | 4 |
CaTi(SiO3)2 (mvc-6468) | 0.4488 | 0.222 | 4 |
LiMn(SiO3)2 (mp-761776) | 0.4115 | 0.202 | 4 |
LiVP2O7 (mp-32476) | 0.4501 | 0.066 | 4 |
LiV(SiO3)2 (mp-766728) | 0.4418 | 0.041 | 4 |
NaPO3 (mp-864891) | 0.3807 | 0.002 | 3 |
MgSiO3 (mp-1020124) | 0.5098 | 0.028 | 3 |
MgSiO3 (mp-1020123) | 0.4668 | 0.039 | 3 |
NaAsO3 (mp-17868) | 0.3791 | 0.002 | 3 |
MgSiO3 (mp-1020115) | 0.5157 | 0.031 | 3 |
Li3MnV(P2O7)2 (mp-850951) | 0.5586 | 0.000 | 5 |
Li3MnV(PO4)3 (mp-780675) | 0.5647 | 0.222 | 5 |
NaLiCu(PO3)3 (mp-775900) | 0.4928 | 0.087 | 5 |
Li6MnV3(PO4)6 (mp-778914) | 0.5667 | 0.228 | 5 |
Li6MnV3(PO4)6 (mp-779387) | 0.5544 | 0.232 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.7151 | 0.080 | 6 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.7015 | 0.085 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.6954 | 0.778 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.7020 | 0.081 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6911 | 0.008 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7081 | 0.068 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv P O |
Final Energy/Atom-6.5427 eV |
Corrected Energy-208.9230 eV
-208.9230 eV = -196.2818 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)