material

Mg3Sc

ID:

mp-864937

DOI:

10.17188/1310246


Material Details

Final Magnetic Moment
0.013 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.034 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.005 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.13 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mg3Sc
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.000 32.9
ZnO (mp-2133) <0 0 1> <0 0 1> 0.003 252.3
SiC (mp-7631) <0 0 1> <0 0 1> 0.003 108.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.004 108.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.007 324.4
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.008 108.1
GaN (mp-804) <1 0 1> <1 0 0> 0.008 230.1
GaN (mp-804) <0 0 1> <0 0 1> 0.013 36.0
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.015 360.4
CdS (mp-672) <0 0 1> <0 0 1> 0.024 108.1
KCl (mp-23193) <1 0 0> <1 0 0> 0.038 164.4
PbS (mp-21276) <1 1 1> <0 0 1> 0.042 252.3
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.043 263.0
CsI (mp-614603) <1 1 1> <0 0 1> 0.043 108.1
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.044 263.0
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.047 144.2
C (mp-66) <1 1 0> <1 0 0> 0.048 164.4
Fe2O3 (mp-24972) <1 0 1> <1 0 0> 0.048 295.8
C (mp-66) <1 0 0> <1 0 0> 0.049 230.1
TiO2 (mp-390) <1 0 0> <1 0 1> 0.049 146.3
C (mp-48) <0 0 1> <0 0 1> 0.062 144.2
Fe2O3 (mp-24972) <1 0 0> <1 1 0> 0.066 284.7
InP (mp-20351) <1 1 0> <1 1 1> 0.074 202.1
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.079 65.7
BN (mp-984) <0 0 1> <1 1 1> 0.079 269.5
PbS (mp-21276) <1 1 0> <1 1 1> 0.082 202.1
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.087 146.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.088 108.1
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.092 243.9
Mg (mp-153) <1 0 1> <1 0 0> 0.099 230.1
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.102 324.4
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.111 252.3
WS2 (mp-224) <1 0 0> <0 0 1> 0.113 180.2
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.116 230.1
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.117 180.2
SiC (mp-11714) <1 0 0> <1 1 0> 0.121 341.6
YAlO3 (mp-3792) <1 1 0> <1 0 1> 0.122 341.5
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.126 284.7
MgO (mp-1265) <1 1 0> <1 1 1> 0.127 202.1
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.127 252.3
KCl (mp-23193) <1 1 0> <1 0 0> 0.131 230.1
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.137 131.5
AlN (mp-661) <0 0 1> <0 0 1> 0.141 108.1
AlN (mp-661) <1 1 0> <1 0 0> 0.141 164.4
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.154 263.0
TiO2 (mp-390) <0 0 1> <1 0 0> 0.171 295.8
BN (mp-984) <1 0 1> <1 0 0> 0.171 164.4
Cu (mp-30) <1 1 1> <1 0 0> 0.172 230.1
NaCl (mp-22862) <1 1 0> <0 0 1> 0.176 180.2
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.177 288.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
73 35 22 0 0 0
35 73 22 0 0 0
22 22 88 0 0 0
0 0 0 20 0 0
0 0 0 0 20 0
0 0 0 0 0 19
Compliance Tensor Sij (10-12Pa-1)
18.4 -8.1 -2.5 0 0 0
-8.1 18.4 -2.5 0 0 0
-2.5 -2.5 12.6 0 0 0
0 0 0 49.6 0 0
0 0 0 0 49.6 0
0 0 0 0 0 52.9
Shear Modulus GV
22 GPa
Bulk Modulus KV
43 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
43 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
43 GPa
Elastic Anisotropy
0.23
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo15W2 (mp-767372) 0.2737 0.028 4
CrFeCoNi (mp-1012640) 0.1479 0.065 4
CrFeCoNi (mp-1096923) 0.3904 0.193 4
Sm3Tm (mp-979973) 0.0142 0.020 2
Sm3Er (mp-979614) 0.0145 0.022 2
Ni3S (mp-976881) 0.0104 0.371 2
YZr (mp-971933) 0.0046 0.113 2
PmHo (mp-973796) 0.0136 0.026 2
Be (mp-87) 0.0042 0.000 1
Ru (mp-33) 0.0037 0.000 1
Os (mp-49) 0.0035 0.000 1
Fe (mp-136) 0.0089 0.098 1
Sc (mp-1057622) 0.0157 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Sc_sv
Final Energy/Atom
-2.8177 eV
Corrected Energy
-22.5418 eV
Uncorrected energy = -22.5418 eV Corrected energy = -22.5418 eV

Detailed input parameters and outputs for all calculations