material

MnAlOs2

ID:

mp-864951

DOI:

10.17188/1310269


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-0.261 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.24 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.000 144.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.000 36.0
PbS (mp-21276) <1 1 0> <1 1 0> 0.000 50.9
PbS (mp-21276) <1 1 1> <1 1 1> 0.000 62.4
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.003 152.8
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.022 216.2
GaN (mp-804) <0 0 1> <1 1 1> 0.033 62.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.034 72.1
MgO (mp-1265) <1 0 0> <1 0 0> 0.041 36.0
MgO (mp-1265) <1 1 0> <1 1 0> 0.044 50.9
MgO (mp-1265) <1 1 1> <1 0 0> 0.069 252.2
ZnO (mp-2133) <1 0 1> <1 0 0> 0.081 216.2
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.094 305.7
C (mp-48) <0 0 1> <1 0 0> 0.098 252.2
KCl (mp-23193) <1 0 0> <1 0 0> 0.102 324.2
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.124 252.2
SiC (mp-11714) <0 0 1> <1 0 0> 0.127 288.2
SiC (mp-7631) <0 0 1> <1 0 0> 0.137 288.2
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.138 72.1
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.142 324.2
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.148 101.9
WS2 (mp-224) <0 0 1> <1 1 1> 0.161 62.4
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.163 62.4
NaCl (mp-22862) <1 0 0> <1 0 0> 0.165 288.2
ZnO (mp-2133) <0 0 1> <1 1 1> 0.244 249.6
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.257 252.2
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.266 144.1
InP (mp-20351) <1 0 0> <1 0 0> 0.280 36.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.286 203.8
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.292 249.6
InP (mp-20351) <1 1 0> <1 1 0> 0.301 50.9
InP (mp-20351) <1 1 1> <1 1 1> 0.308 62.4
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.312 180.1
ZnO (mp-2133) <1 0 0> <1 1 1> 0.313 312.0
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.335 252.2
Ni (mp-23) <1 0 0> <1 1 0> 0.365 254.7
CdS (mp-672) <0 0 1> <1 1 1> 0.421 62.4
Al (mp-134) <1 0 0> <1 0 0> 0.434 144.1
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.451 360.3
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.463 152.8
Al (mp-134) <1 1 0> <1 1 0> 0.466 203.8
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.474 187.2
Al (mp-134) <1 1 1> <1 1 1> 0.476 249.6
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.494 324.2
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.513 324.2
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.529 360.3
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.544 152.8
AlN (mp-661) <1 0 1> <1 1 0> 0.545 254.7
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.548 187.2
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.565 180.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
391 192 192 0 0 0
192 391 192 0 0 0
192 192 391 0 0 0
0 0 0 184 0 0
0 0 0 0 184 0
0 0 0 0 0 184
Compliance Tensor Sij (10-12Pa-1)
3.8 -1.2 -1.2 0 0 0
-1.2 3.8 -1.2 0 0 0
-1.2 -1.2 3.8 0 0 0
0 0 0 5.4 0 0
0 0 0 0 5.4 0
0 0 0 0 0 5.4
Shear Modulus GV
150 GPa
Bulk Modulus KV
258 GPa
Shear Modulus GR
138 GPa
Bulk Modulus KR
258 GPa
Shear Modulus GVRH
144 GPa
Bulk Modulus KVRH
258 GPa
Elastic Anisotropy
0.47
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sc2CdIn (mp-862711) 0.0000 0.000 3
MnAlIr2 (mp-864950) 0.0000 0.000 3
LuZrRu2 (mp-865434) 0.0000 0.000 3
YbPmAg2 (mp-865896) 0.0000 0.000 3
Tb2IrRu (mp-867291) 0.0000 0.032 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
LiMgSbPt (mp-571584) 0.0000 0.086 4
LiMgSbPd (mp-10179) 0.0000 0.074 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
Rb3Sn (mp-974789) 0.0000 0.152 2
LiCd3 (mp-973940) 0.0000 0.000 2
Rb3Sm (mp-974816) 0.0000 0.631 2
SmAg3 (mp-862736) 0.0000 0.034 2
Rb3Ho (mp-974962) 0.0000 0.641 2
Br (mp-673171) 0.0000 0.630 1
Ti (mp-73) 0.0000 0.112 1
I (mp-684663) 0.0000 0.446 1
Cr (mp-90) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.139 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Al Os_pv
Final Energy/Atom
-9.1019 eV
Corrected Energy
-72.8150 eV
-72.8150 eV = -72.8150 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)