material

Mg3Ag

ID:

mp-864952

DOI:

10.17188/1310270


Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.119 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.020 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mg149Ag + MgAg
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.000 32.9
BaTiO3 (mp-5986) <1 0 1> <1 1 1> 0.001 186.0
Ge (mp-32) <1 1 1> <0 0 1> 0.002 230.6
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.002 296.5
Te2W (mp-22693) <1 1 0> <1 0 1> 0.003 223.9
GdScO3 (mp-5690) <1 0 0> <1 1 1> 0.004 186.0
C (mp-48) <1 1 1> <1 0 0> 0.010 303.2
YVO4 (mp-19133) <0 0 1> <1 0 1> 0.011 313.4
SiC (mp-8062) <1 0 0> <1 0 1> 0.011 134.3
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.012 164.7
GaAs (mp-2534) <1 1 1> <0 0 1> 0.015 230.6
SiC (mp-11714) <0 0 1> <0 0 1> 0.016 32.9
Cu (mp-30) <1 1 1> <0 0 1> 0.016 296.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.018 32.9
TiO2 (mp-390) <0 0 1> <0 0 1> 0.021 230.6
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.022 230.6
SiC (mp-8062) <1 1 1> <0 0 1> 0.025 32.9
InSb (mp-20012) <1 1 1> <0 0 1> 0.026 230.6
SiC (mp-11714) <1 1 0> <1 0 0> 0.028 272.9
InAs (mp-20305) <1 0 0> <1 0 0> 0.029 151.6
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.030 230.6
TbScO3 (mp-31119) <1 0 0> <1 1 1> 0.031 186.0
CdTe (mp-406) <1 1 1> <0 0 1> 0.034 230.6
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.036 151.6
Mg (mp-153) <1 0 1> <0 0 1> 0.040 362.4
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.042 313.4
Ni (mp-23) <1 1 1> <1 0 0> 0.048 212.2
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.048 197.7
DyScO3 (mp-31120) <1 1 1> <1 1 0> 0.048 210.1
TiO2 (mp-390) <1 1 0> <1 1 1> 0.060 310.0
C (mp-48) <0 0 1> <0 0 1> 0.064 98.8
DyScO3 (mp-31120) <1 0 0> <1 1 1> 0.065 186.0
C (mp-48) <1 0 1> <1 1 0> 0.066 157.6
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.077 230.6
BN (mp-984) <1 1 1> <1 0 0> 0.084 272.9
AlN (mp-661) <0 0 1> <1 0 1> 0.085 134.3
ZnO (mp-2133) <0 0 1> <0 0 1> 0.087 230.6
ZnSe (mp-1190) <1 1 0> <1 1 1> 0.089 186.0
TbScO3 (mp-31119) <1 1 1> <1 1 0> 0.089 210.1
AlN (mp-661) <1 0 1> <1 0 0> 0.093 212.2
GaAs (mp-2534) <1 1 0> <1 1 1> 0.096 186.0
C (mp-48) <1 0 0> <1 0 0> 0.096 151.6
Ni (mp-23) <1 1 0> <1 1 0> 0.103 52.5
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.103 151.6
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.104 164.7
Ni (mp-23) <1 0 0> <1 1 0> 0.105 262.6
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.109 262.6
ZnO (mp-2133) <1 0 0> <1 0 1> 0.109 223.9
CdS (mp-672) <0 0 1> <0 0 1> 0.113 296.5
GaSe (mp-1943) <0 0 1> <1 0 0> 0.114 333.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
74 37 28 0 0 0
37 74 28 0 0 0
28 28 98 0 0 0
0 0 0 23 0 0
0 0 0 0 23 0
0 0 0 0 0 19
Compliance Tensor Sij (10-12Pa-1)
18.5 -8 -3 0 0 0
-8 18.5 -3 0 0 0
-3 -3 11.9 0 0 0
0 0 0 43.1 0 0
0 0 0 0 43.1 0
0 0 0 0 0 53.1
Shear Modulus GV
23 GPa
Bulk Modulus KV
48 GPa
Shear Modulus GR
22 GPa
Bulk Modulus KR
48 GPa
Shear Modulus GVRH
23 GPa
Bulk Modulus KVRH
48 GPa
Elastic Anisotropy
0.21
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo15W2 (mp-767372) 0.2584 0.028 4
CrFeCoNi (mp-1012640) 0.0901 0.065 4
CrFeCoNi (mp-1096923) 0.3452 0.193 4
Pm3Sc (mp-976797) 0.0266 0.042 2
ReAg3 (mp-974525) 0.0362 0.894 2
Ho3Mg (mp-974322) 0.0287 0.046 2
LiCd3 (mp-865612) 0.0335 0.001 2
Y3Mg (mp-1094397) 0.0263 0.054 2
Pr (mp-1059256) 0.1107 0.029 1
Y (mp-1059189) 0.1075 0.004 1
Ru (mp-33) 0.1197 0.000 1
Os (mp-49) 0.1201 0.000 1
Ca (mp-1064227) 0.1056 0.007 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Ag
Final Energy/Atom
-2.0271 eV
Corrected Energy
-16.2170 eV
Uncorrected energy = -16.2170 eV Corrected energy = -16.2170 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)