material

MnV2Cr

ID:

mp-864953

DOI:

10.17188/1310271


Material Details

Final Magnetic Moment
0.104 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.189 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.15 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <1 1 1> 0.000 58.0
SiC (mp-7631) <0 0 1> <1 1 1> 0.000 58.0
SiC (mp-8062) <1 1 1> <1 1 1> 0.003 232.1
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.014 94.8
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.015 268.0
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.015 67.0
Si (mp-149) <1 0 0> <1 0 0> 0.019 268.0
LiF (mp-1138) <1 1 0> <1 1 0> 0.022 47.4
LiF (mp-1138) <1 0 0> <1 0 0> 0.023 33.5
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.030 94.8
MoSe2 (mp-1634) <1 1 0> <1 0 0> 0.030 268.0
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.046 134.0
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.048 167.5
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.061 174.1
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.074 167.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.074 284.3
Ge (mp-32) <1 1 1> <1 1 1> 0.075 58.0
C (mp-66) <1 0 0> <1 0 0> 0.076 167.5
Ge (mp-32) <1 1 0> <1 1 0> 0.077 47.4
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.078 142.2
Ge (mp-32) <1 0 0> <1 0 0> 0.083 33.5
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.084 234.5
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.085 94.8
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.120 142.2
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.151 167.5
GaAs (mp-2534) <1 1 1> <1 1 1> 0.167 58.0
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.168 94.8
GaAs (mp-2534) <1 1 0> <1 1 0> 0.171 47.4
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.174 268.0
GaAs (mp-2534) <1 0 0> <1 0 0> 0.185 33.5
InAs (mp-20305) <1 0 0> <1 0 0> 0.201 301.5
AlN (mp-661) <0 0 1> <1 1 0> 0.209 236.9
GaSe (mp-1943) <0 0 1> <1 1 0> 0.213 189.5
GaTe (mp-542812) <1 0 -1> <1 0 0> 0.217 301.5
InSb (mp-20012) <1 1 1> <1 1 1> 0.220 232.1
InSb (mp-20012) <1 1 0> <1 1 0> 0.226 189.5
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.227 301.5
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.234 301.5
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.242 58.0
WS2 (mp-224) <1 1 0> <1 1 1> 0.248 232.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.249 47.4
CdTe (mp-406) <1 1 1> <1 1 1> 0.258 232.1
CdTe (mp-406) <1 1 0> <1 1 0> 0.264 189.5
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.266 268.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.268 33.5
Mg (mp-153) <1 1 1> <1 0 0> 0.271 268.0
BN (mp-984) <0 0 1> <1 1 0> 0.277 189.5
C (mp-66) <1 1 0> <1 1 0> 0.285 142.2
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.292 232.1
LiF (mp-1138) <1 1 1> <1 0 0> 0.294 234.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
435 129 129 0 -0 0
129 435 129 0 -0 0
129 129 435 0 -0 0
0 0 0 73 0 -0
-0 -0 -0 0 73 0
0 0 0 -0 0 73
Compliance Tensor Sij (10-12Pa-1)
2.7 -0.6 -0.6 0 0 0
-0.6 2.7 -0.6 0 0 0
-0.6 -0.6 2.7 0 0 0
0 0 0 13.7 0 0
0 0 0 0 13.7 0
0 0 0 0 0 13.7
Shear Modulus GV
105 GPa
Bulk Modulus KV
231 GPa
Shear Modulus GR
92 GPa
Bulk Modulus KR
231 GPa
Shear Modulus GVRH
99 GPa
Bulk Modulus KVRH
231 GPa
Elastic Anisotropy
0.69
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSbPt (mp-571584) 0.0000 0.080 4
TiFeCoAs (mp-998974) 0.0000 0.146 4
LiMgSbPd (mp-10179) 0.0000 0.067 4
MnGaFeCo (mp-999552) 0.0000 0.045 4
Yb3Mn (mp-979955) 0.0000 0.311 2
Si3Ge (mp-972751) 0.0000 0.539 2
K3Hg (mp-983388) 0.0000 0.061 2
K3Sn (mp-973614) 0.0000 0.105 2
LiCd3 (mp-973940) 0.0000 0.015 2
NaInHg2 (mp-865100) 0.0000 0.000 3
PrMgAg2 (mp-975892) 0.0000 0.000 3
Pm2ZnOs (mp-983236) 0.0000 0.000 3
Pr2SnHg (mp-861510) 0.0000 0.000 3
Er2ZnCu (mp-983583) 0.0000 0.009 3
Be (mp-20) 0.0000 0.108 1
Nb (mp-75) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.153 1
Br (mp-673171) 0.0000 0.616 1
I (mp-684663) 0.0000 0.455 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv V_pv Cr_pv
Final Energy/Atom
-9.4308 eV
Corrected Energy
-37.7233 eV
-37.7233 eV = -37.7233 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)