Final Magnetic Moment
3.320 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.304 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.76 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic
We have not yet calculated a detailed bandstructure for this material
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 0 0> <1 0 0> 0.001 146.6
Al (mp-134) <1 1 0> <1 1 0> 0.001 207.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.006 146.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.006 207.4
Ag (mp-124) <1 0 0> <1 0 0> 0.009 293.3
C (mp-48) <0 0 1> <1 1 1> 0.011 63.5
ZnO (mp-2133) <0 0 1> <1 1 1> 0.014 254.0
NaCl (mp-22862) <1 0 0> <1 0 0> 0.025 293.3
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.034 155.5
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.035 73.3
C (mp-66) <1 0 0> <1 0 0> 0.037 329.9
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.039 103.7
Ni (mp-23) <1 1 0> <1 1 0> 0.044 51.8
Ni (mp-23) <1 1 1> <1 1 1> 0.046 63.5
Ni (mp-23) <1 0 0> <1 1 0> 0.051 259.2
KCl (mp-23193) <1 0 0> <1 0 0> 0.051 329.9
Au (mp-81) <1 0 0> <1 0 0> 0.057 293.3
ZnO (mp-2133) <1 0 1> <1 0 0> 0.065 219.9
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.099 293.3
MgO (mp-1265) <1 0 0> <1 0 0> 0.101 36.7
Mg (mp-153) <1 0 0> <1 0 0> 0.106 183.3
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.109 293.3
TiO2 (mp-390) <0 0 1> <1 0 0> 0.110 73.3
SiC (mp-7631) <0 0 1> <1 0 0> 0.111 293.3
MgO (mp-1265) <1 1 0> <1 1 0> 0.113 51.8
SiC (mp-11714) <0 0 1> <1 0 0> 0.120 293.3
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.122 155.5
C (mp-66) <1 1 0> <1 1 0> 0.131 311.0
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.133 183.3
GaN (mp-804) <0 0 1> <1 1 1> 0.135 63.5
AlN (mp-661) <0 0 1> <1 0 0> 0.142 293.3
GaN (mp-804) <1 0 0> <1 0 0> 0.143 183.3
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.151 110.0
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.157 190.5
GaAs (mp-2534) <1 0 0> <1 0 0> 0.166 293.3
C (mp-48) <1 1 0> <1 0 0> 0.191 329.9
SiC (mp-11714) <1 0 1> <1 0 0> 0.205 256.6
PbS (mp-21276) <1 0 0> <1 0 0> 0.216 36.7
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.218 110.0
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.218 146.6
ZnO (mp-2133) <1 0 0> <1 1 1> 0.218 317.5
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.222 155.5
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.232 329.9
PbS (mp-21276) <1 1 0> <1 1 0> 0.244 51.8
PbS (mp-21276) <1 1 1> <1 1 1> 0.253 63.5
ZnO (mp-2133) <1 1 0> <1 0 0> 0.259 329.9
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.263 207.4
LaF3 (mp-905) <1 0 0> <1 1 1> 0.265 317.5
Au (mp-81) <1 1 1> <1 0 0> 0.266 183.3
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.266 311.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
199 153 153 0 0 -0
153 199 153 -0 0 0
153 153 199 0 -0 0
0 -0 0 112 0 0
0 0 -0 0 112 0
-0 0 0 0 0 112
Compliance Tensor Sij (10-12Pa-1)
15.1 -6.6 -6.6 0 0 0
-6.6 15.1 -6.6 0 0 0
-6.6 -6.6 15.1 0 0 0
0 0 0 9 0 0
0 0 0 0 9 0
0 0 0 0 0 9
Shear Modulus GV
76 GPa
Bulk Modulus KV
168 GPa
Shear Modulus GR
44 GPa
Bulk Modulus KR
168 GPa
Shear Modulus GVRH
60 GPa
Bulk Modulus KVRH
168 GPa
Elastic Anisotropy
3.65
Poisson's Ratio
0.34

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
28
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Zn Rh_pv
Final Energy/Atom
-6.5867 eV
Corrected Energy
-26.3469 eV
-26.3469 eV = -26.3469 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)