material

CaB6

ID:

mp-865

DOI:

10.17188/1310320


Tags: Calcium octahedro-hexaboride (1/1) Calcium hexaboride Calcium boride (1/6)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.408 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.44 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.184 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 26753 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.000 155.0
PbSe (mp-2201) <1 1 0> <1 1 0> 0.000 219.2
PbSe (mp-2201) <1 0 0> <1 0 0> 0.000 155.0
TePb (mp-19717) <1 0 0> <1 0 0> 0.001 86.1
GaSb (mp-1156) <1 1 0> <1 1 0> 0.002 219.2
GaSb (mp-1156) <1 0 0> <1 0 0> 0.003 155.0
CdSe (mp-2691) <1 1 0> <1 1 0> 0.009 219.2
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.011 223.9
CdSe (mp-2691) <1 0 0> <1 0 0> 0.011 155.0
SiC (mp-11714) <1 0 0> <1 1 0> 0.011 219.2
Ag (mp-124) <1 1 1> <1 1 1> 0.013 29.8
Ag (mp-124) <1 1 0> <1 1 0> 0.014 24.4
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.018 119.3
Ag (mp-124) <1 0 0> <1 0 0> 0.018 17.2
GaP (mp-2490) <1 1 1> <1 1 1> 0.018 208.8
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.018 86.1
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.021 310.0
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.021 137.8
Si (mp-149) <1 1 1> <1 1 1> 0.031 208.8
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.035 208.8
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.038 137.8
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.047 208.8
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.049 219.2
Mg (mp-153) <1 0 1> <1 0 0> 0.050 206.7
SiC (mp-11714) <1 1 0> <1 1 0> 0.052 219.2
Au (mp-81) <1 1 1> <1 1 1> 0.055 29.8
SiC (mp-8062) <1 1 0> <1 1 0> 0.058 219.2
Au (mp-81) <1 1 0> <1 1 0> 0.059 24.4
C (mp-66) <1 1 1> <1 1 1> 0.061 89.5
C (mp-66) <1 1 0> <1 1 0> 0.066 73.1
C (mp-48) <1 0 1> <1 1 0> 0.068 316.6
Te2W (mp-22693) <0 1 1> <1 1 0> 0.070 292.3
GaTe (mp-542812) <1 0 1> <1 1 0> 0.070 97.4
SiC (mp-8062) <1 0 0> <1 0 0> 0.071 155.0
Au (mp-81) <1 0 0> <1 0 0> 0.074 17.2
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.074 89.5
Cu (mp-30) <1 1 1> <1 1 1> 0.081 89.5
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.084 155.0
C (mp-48) <1 1 1> <1 1 0> 0.084 170.5
GaSe (mp-1943) <0 0 1> <1 1 1> 0.085 89.5
Cu (mp-30) <1 1 0> <1 1 0> 0.088 73.1
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.094 219.2
AlN (mp-661) <1 1 0> <1 1 0> 0.105 219.2
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.109 267.9
InAs (mp-20305) <1 1 0> <1 1 0> 0.110 219.2
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.117 155.0
Mg (mp-153) <1 1 1> <1 0 0> 0.120 275.6
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.124 155.0
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.124 73.1
InAs (mp-20305) <1 0 0> <1 0 0> 0.137 155.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
432 8 8 0 0 0
8 432 8 0 0 0
8 8 432 0 0 0
0 0 0 42 0 0
0 0 0 0 42 0
0 0 0 0 0 42
Compliance Tensor Sij (10-12Pa-1)
2.3 0 0 0 0 0
0 2.3 0 0 0 0
0 0 2.3 0 0 0
0 0 0 23.7 0 0
0 0 0 0 23.7 0
0 0 0 0 0 23.7
Shear Modulus GV
110 GPa
Bulk Modulus KV
149 GPa
Shear Modulus GR
62 GPa
Bulk Modulus KR
149 GPa
Shear Modulus GVRH
86 GPa
Bulk Modulus KVRH
149 GPa
Elastic Anisotropy
3.88
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
EuB6 (mp-20874) 0.0119 0.000 2
BiB6 (mp-1096844) 0.0043 0.339 2
YbB6 (mp-419) 0.0057 0.000 2
SnB6 (mp-1094049) 0.0086 0.174 2
EuB6 (mp-1077914) 0.0077 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv B
Final Energy/Atom
-6.4195 eV
Corrected Energy
-44.9366 eV
-44.9366 eV = -44.9366 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 196516
  • 194632
  • 612684
  • 612687
  • 26753
  • 44985
  • 655040
  • 612689
  • 612682
  • 26893
Submitted by
User remarks:
  • Calcium hexaboride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)