material

HfScOs2

ID:

mp-865001

DOI:

10.17188/1310322


Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.566 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.79 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <0 0 1> <1 1 1> 0.000 290.3
Ni (mp-23) <1 0 0> <1 0 0> 0.002 209.5
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.007 209.5
CdS (mp-672) <0 0 1> <1 1 1> 0.011 290.3
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.021 290.3
LiF (mp-1138) <1 0 0> <1 0 0> 0.032 83.8
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.046 209.5
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.054 335.2
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.054 335.2
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.065 177.8
C (mp-66) <1 1 1> <1 1 1> 0.096 290.3
C (mp-66) <1 0 0> <1 0 0> 0.096 167.6
MgO (mp-1265) <1 1 1> <1 1 1> 0.099 217.7
Ge (mp-32) <1 0 0> <1 0 0> 0.104 167.6
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.115 177.8
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.121 290.3
CdS (mp-672) <1 1 1> <1 0 0> 0.170 209.5
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.170 145.1
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.193 209.5
C (mp-48) <0 0 1> <1 1 0> 0.208 237.0
GaAs (mp-2534) <1 0 0> <1 0 0> 0.226 167.6
Cu (mp-30) <1 1 1> <1 1 1> 0.257 290.3
Cu (mp-30) <1 0 0> <1 0 0> 0.259 167.6
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.267 118.5
SiC (mp-11714) <0 0 1> <1 1 0> 0.281 296.3
WS2 (mp-224) <0 0 1> <1 1 0> 0.282 177.8
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.283 177.8
GaN (mp-804) <0 0 1> <1 1 0> 0.292 177.8
SiC (mp-7631) <0 0 1> <1 1 0> 0.293 296.3
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.325 167.6
BN (mp-984) <1 0 1> <1 1 1> 0.347 217.7
CsI (mp-614603) <1 1 0> <1 1 0> 0.363 177.8
Mg (mp-153) <0 0 1> <1 1 0> 0.387 177.8
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.387 177.8
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.389 177.8
Ni (mp-23) <1 1 0> <1 0 0> 0.391 335.2
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.443 251.4
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.444 217.7
AlN (mp-661) <1 0 1> <1 1 0> 0.474 177.8
TiO2 (mp-390) <1 0 1> <1 1 0> 0.509 118.5
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.520 167.6
ZnO (mp-2133) <1 0 0> <1 0 0> 0.534 209.5
YAlO3 (mp-3792) <1 0 1> <1 1 1> 0.548 145.1
SiC (mp-11714) <1 0 1> <1 0 0> 0.553 293.3
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.628 237.0
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.631 290.3
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.662 237.0
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.669 72.6
KCl (mp-23193) <1 1 1> <1 1 1> 0.696 72.6
KCl (mp-23193) <1 1 0> <1 1 0> 0.697 59.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
329 137 137 0 -0 0
137 329 137 0 0 -0
137 137 329 -0 0 0
0 0 -0 91 0 0
-0 0 0 0 91 0
0 -0 0 0 0 91
Compliance Tensor Sij (10-12Pa-1)
4 -1.2 -1.2 0 0 0
-1.2 4 -1.2 0 0 0
-1.2 -1.2 4 0 0 0
0 0 0 10.9 0 0
0 0 0 0 10.9 0
0 0 0 0 0 10.9
Shear Modulus GV
93 GPa
Bulk Modulus KV
201 GPa
Shear Modulus GR
93 GPa
Bulk Modulus KR
201 GPa
Shear Modulus GVRH
93 GPa
Bulk Modulus KVRH
201 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMgSnPt (mp-11806) 0.0000 0.000 4
LiMgSbPt (mp-571584) 0.0000 0.080 4
TiFeCoAs (mp-998974) 0.0000 0.146 4
LiMgSnAu (mp-7554) 0.0000 0.063 4
MnGaFeCo (mp-999552) 0.0000 0.045 4
Na3Pu (mp-1006151) 0.0000 0.548 2
Li3In (mp-867226) 0.0000 0.000 2
SmAg3 (mp-862736) 0.0000 0.000 2
ZnHg3 (mp-971757) 0.0000 0.126 2
V3Cu (mp-979283) 0.0000 0.162 2
ScRh2Pb (mp-862629) 0.0000 0.000 3
LiLa2Os (mp-867813) 0.0000 0.000 3
TmHfOs2 (mp-865209) 0.0000 0.000 3
Sm2ZnRu (mp-867921) 0.0000 0.000 3
YbAcHg2 (mp-866203) 0.0000 0.000 3
Ta (mp-50) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.153 1
Cr (mp-90) 0.0000 0.000 1
I (mp-684663) 0.0000 0.455 1
Tl (mp-39) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Sc_sv Os_pv
Final Energy/Atom
-10.2480 eV
Corrected Energy
-40.9919 eV
-40.9919 eV = -40.9919 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)