material

Mg2Cu

ID:

mp-865014

DOI:

10.17188/1310334


Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.104 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.017 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.37 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mg2Cu
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Ibam [72]
Hall
-I 2 2c
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YAlO3 (mp-3792) <0 1 1> <0 1 1> 0.004 48.2
Ge (mp-32) <1 1 0> <1 1 0> 0.006 329.2
YAlO3 (mp-3792) <0 0 1> <0 1 0> 0.010 140.5
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.013 213.9
C (mp-48) <1 1 0> <1 0 1> 0.016 267.4
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.020 32.9
MoSe2 (mp-1634) <1 0 1> <1 0 0> 0.025 210.7
LaF3 (mp-905) <0 0 1> <1 0 1> 0.028 320.9
Mg (mp-153) <1 0 1> <1 0 0> 0.030 168.6
AlN (mp-661) <1 1 0> <0 1 0> 0.036 351.3
C (mp-48) <1 1 1> <1 0 1> 0.039 267.4
NaCl (mp-22862) <1 1 1> <0 1 1> 0.039 337.1
Te2W (mp-22693) <0 0 1> <0 0 1> 0.039 65.9
TiO2 (mp-390) <1 0 1> <0 0 1> 0.040 197.6
AlN (mp-661) <1 0 0> <1 1 0> 0.045 109.7
GaSe (mp-1943) <0 0 1> <1 0 0> 0.045 126.4
C (mp-48) <1 0 1> <0 0 1> 0.056 98.8
LiGaO2 (mp-5854) <1 1 1> <0 1 0> 0.058 281.0
SiC (mp-11714) <1 0 0> <1 0 0> 0.061 126.4
GaSb (mp-1156) <1 1 0> <0 0 1> 0.064 164.7
PbSe (mp-2201) <1 1 0> <0 0 1> 0.064 164.7
Ag (mp-124) <1 1 0> <0 1 0> 0.065 316.2
AlN (mp-661) <1 1 1> <0 1 0> 0.066 140.5
Al (mp-134) <1 0 0> <1 1 0> 0.067 164.6
CdSe (mp-2691) <1 1 0> <0 0 1> 0.067 164.7
GaN (mp-804) <1 1 0> <0 1 1> 0.068 144.5
BN (mp-984) <1 0 0> <1 0 0> 0.070 210.7
Te2W (mp-22693) <1 0 1> <0 0 1> 0.079 98.8
LiTaO3 (mp-3666) <1 0 0> <0 1 1> 0.082 144.5
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.082 230.5
ZrO2 (mp-2858) <1 0 0> <0 1 0> 0.086 140.5
Al (mp-134) <1 1 0> <0 0 1> 0.092 230.5
Mg (mp-153) <1 0 0> <0 0 1> 0.093 32.9
PbS (mp-21276) <1 0 0> <1 1 1> 0.096 256.0
LiF (mp-1138) <1 0 0> <1 1 0> 0.097 164.6
KTaO3 (mp-3614) <1 0 0> <1 1 0> 0.100 164.6
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.101 230.5
InSb (mp-20012) <1 1 0> <1 0 0> 0.102 126.4
YAlO3 (mp-3792) <0 1 0> <0 1 1> 0.116 192.6
CdTe (mp-406) <1 0 0> <0 1 0> 0.117 175.7
CdTe (mp-406) <1 1 0> <1 0 0> 0.118 126.4
YAlO3 (mp-3792) <1 1 0> <0 1 0> 0.121 281.0
InSb (mp-20012) <1 0 0> <0 1 0> 0.121 175.7
BaF2 (mp-1029) <1 0 0> <1 0 1> 0.126 160.4
WS2 (mp-224) <1 0 0> <1 0 1> 0.128 267.4
MgF2 (mp-1249) <0 0 1> <0 1 0> 0.128 175.7
TiO2 (mp-390) <1 0 0> <0 0 1> 0.132 329.3
MoS2 (mp-1434) <1 0 0> <1 0 1> 0.134 267.4
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.138 329.2
LiF (mp-1138) <1 1 1> <1 0 1> 0.139 320.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
113 25 25 0 0 0
25 83 61 0 0 0
25 61 84 0 0 0
0 0 0 38 0 0
0 0 0 0 33 0
0 0 0 0 0 32
Compliance Tensor Sij (10-12Pa-1)
9.6 -1.7 -1.7 0 0 0
-1.7 25.7 -18.1 0 0 0
-1.7 -18.1 25.6 0 0 0
0 0 0 26.1 0 0
0 0 0 0 30.8 0
0 0 0 0 0 30.8
Shear Modulus GV
32 GPa
Bulk Modulus KV
56 GPa
Shear Modulus GR
25 GPa
Bulk Modulus KR
56 GPa
Shear Modulus GVRH
29 GPa
Bulk Modulus KVRH
56 GPa
Elastic Anisotropy
1.30
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CoP (mp-21447) 0.2367 0.044 3
Nb4SiNi (mp-22396) 0.2633 0.009 3
Ta4FeP (mp-22444) 0.2733 0.055 3
Nb4FeSi (mp-22312) 0.2932 0.048 3
Nb4CoSi (mp-10003) 0.2614 0.013 3
MnSn2 (mp-1077425) 0.2727 0.136 2
Mg2Cu (mp-2481) 0.2561 0.000 2
Zr2Ni (mp-328) 0.2621 0.000 2
Hf2Ni (mp-861) 0.2620 0.005 2
MnSn2 (mp-20086) 0.2609 0.136 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Cu_pv
Final Energy/Atom
-2.5346 eV
Corrected Energy
-15.2075 eV
-15.2075 eV = -15.2075 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by