material

MgInPd2

ID:

mp-865043

DOI:

10.17188/1310360


Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.676 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.53 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.001 211.0
MgO (mp-1265) <1 1 1> <1 1 1> 0.002 219.3
CdS (mp-672) <0 0 1> <1 1 1> 0.012 292.4
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.017 211.0
ZnO (mp-2133) <0 0 1> <1 1 1> 0.030 292.4
Cu (mp-30) <1 0 0> <1 0 0> 0.032 168.8
Cu (mp-30) <1 1 1> <1 1 1> 0.036 292.4
Ni (mp-23) <1 0 0> <1 0 0> 0.044 211.0
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.048 337.6
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.049 337.6
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.055 211.0
GaN (mp-804) <0 0 1> <1 1 0> 0.063 179.0
BN (mp-984) <1 0 1> <1 1 1> 0.065 219.3
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.089 292.4
LiF (mp-1138) <1 0 0> <1 0 0> 0.090 84.4
SiC (mp-7631) <0 0 1> <1 1 0> 0.091 298.4
SiC (mp-11714) <0 0 1> <1 1 0> 0.091 298.4
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.106 211.0
ZnO (mp-2133) <1 0 0> <1 0 0> 0.112 211.0
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.115 292.4
Mg (mp-153) <0 0 1> <1 0 0> 0.120 211.0
GaSe (mp-1943) <0 0 1> <1 0 0> 0.122 126.6
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.122 219.3
C (mp-48) <0 0 1> <1 1 0> 0.127 238.7
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.128 211.0
WS2 (mp-224) <0 0 1> <1 0 0> 0.128 211.0
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.141 179.0
CdS (mp-672) <1 1 1> <1 0 0> 0.148 211.0
C (mp-66) <1 0 0> <1 0 0> 0.154 168.8
Ge (mp-32) <1 0 0> <1 0 0> 0.161 168.8
Te2W (mp-22693) <1 0 0> <1 0 0> 0.165 295.4
C (mp-66) <1 1 1> <1 1 1> 0.176 292.4
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.185 238.7
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.186 292.4
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.187 146.2
YAlO3 (mp-3792) <1 0 1> <1 1 1> 0.187 146.2
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.189 219.3
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.190 179.0
MgF2 (mp-1249) <1 1 1> <1 1 0> 0.192 59.7
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.201 292.4
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.208 295.4
InAs (mp-20305) <1 0 0> <1 0 0> 0.212 337.6
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.214 211.0
Te2W (mp-22693) <0 0 1> <1 1 0> 0.229 179.0
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.238 337.6
LaAlO3 (mp-2920) <1 0 1> <1 1 0> 0.243 298.4
LaF3 (mp-905) <1 0 0> <1 0 0> 0.245 211.0
BN (mp-984) <0 0 1> <1 0 0> 0.256 211.0
GaAs (mp-2534) <1 0 0> <1 0 0> 0.258 168.8
TePb (mp-19717) <1 0 0> <1 0 0> 0.287 42.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
128 99 99 -0 0 0
99 128 99 0 -0 0
99 99 128 0 0 -0
-0 0 0 63 0 0
0 -0 0 0 63 0
0 0 -0 0 0 63
Compliance Tensor Sij (10-12Pa-1)
24.6 -10.8 -10.8 0 0 0
-10.8 24.6 -10.8 0 0 0
-10.8 -10.8 24.6 0 0 0
0 0 0 15.8 0 0
0 0 0 0 15.8 0
0 0 0 0 0 15.8
Shear Modulus GV
44 GPa
Bulk Modulus KV
109 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
109 GPa
Shear Modulus GVRH
35 GPa
Bulk Modulus KVRH
109 GPa
Elastic Anisotropy
3.24
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMgSnPt (mp-11806) 0.0000 0.000 4
LiMgSbPt (mp-571584) 0.0000 0.080 4
TiFeCoAs (mp-998974) 0.0000 0.146 4
LiMgSnAu (mp-7554) 0.0000 0.063 4
MnGaFeCo (mp-999552) 0.0000 0.045 4
Na3Pu (mp-1006151) 0.0000 0.548 2
Li3In (mp-867226) 0.0000 0.000 2
SmAg3 (mp-862736) 0.0000 0.000 2
ZnHg3 (mp-971757) 0.0000 0.126 2
V3Cu (mp-979283) 0.0000 0.162 2
SmMgZn2 (mp-867871) 0.0000 0.000 3
SmSnAu2 (mp-972526) 0.0000 0.000 3
TbSnRh2 (mp-864600) 0.0000 0.000 3
EuAcAu2 (mp-1006278) 0.0000 0.000 3
YbAcHg2 (mp-866203) 0.0000 0.000 3
Ta (mp-50) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.153 1
Cr (mp-90) 0.0000 0.000 1
I (mp-684663) 0.0000 0.455 1
Tl (mp-39) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv In_d Pd
Final Energy/Atom
-4.3494 eV
Corrected Energy
-17.3974 eV
-17.3974 eV = -17.3974 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations