Final Magnetic Moment1.052 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.504 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeAu + Na2Au + CeAu2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 294.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 156.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 147.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 270.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 312.5 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 270.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 260.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 208.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 260.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 260.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 147.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 208.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 260.4 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 260.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 52.1 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 221.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 221.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 73.7 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 90.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 260.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 156.2 |
Al (mp-134) | <1 0 0> | <1 0 0> | 208.3 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 208.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 294.6 |
C (mp-66) | <1 1 0> | <1 1 0> | 73.7 |
C (mp-66) | <1 1 1> | <1 1 1> | 90.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 294.6 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 260.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 260.4 |
InP (mp-20351) | <1 1 1> | <1 1 0> | 294.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 260.4 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 208.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 294.6 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 260.4 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 208.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 221.0 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 221.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 260.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 260.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 294.6 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 260.4 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 221.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 260.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 208.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 221.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 221.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 221.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 270.6 |
Si (mp-149) | <1 0 0> | <1 0 0> | 260.4 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 270.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
27 | -6 | -6 | 0 | 0 | 0 |
-6 | 27 | -6 | 0 | 0 | 0 |
-6 | -6 | 27 | 0 | 0 | 0 |
0 | 0 | 0 | 19 | 0 | 0 |
0 | 0 | 0 | 0 | 19 | 0 |
0 | 0 | 0 | 0 | 0 | 19 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
41.5 | 11.3 | 11.3 | 0 | 0 | 0 |
11.3 | 41.5 | 11.3 | 0 | 0 | 0 |
11.3 | 11.3 | 41.5 | 0 | 0 | 0 |
0 | 0 | 0 | 53.5 | 0 | 0 |
0 | 0 | 0 | 0 | 53.5 | 0 |
0 | 0 | 0 | 0 | 0 | 53.5 |
Shear Modulus GV18 GPa |
Bulk Modulus KV5 GPa |
Shear Modulus GR18 GPa |
Bulk Modulus KR5 GPa |
Shear Modulus GVRH18 GPa |
Bulk Modulus KVRH5 GPa |
Elastic Anisotropy0.02 |
Poisson's Ratio-0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YErTl2 (mp-981548) | 0.0000 | 0.000 | 3 |
TbAlAg2 (mp-977394) | 0.0000 | 0.006 | 3 |
NdLuMg2 (mp-975515) | 0.0000 | 0.009 | 3 |
Li2AcTl (mp-976333) | 0.0000 | 0.000 | 3 |
KSc2Co (mp-631466) | 0.0000 | 1.151 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.163 | 4 |
Sn3B (mp-978917) | 0.0000 | 0.937 | 2 |
MgSn3 (mp-1094230) | 0.0000 | 0.091 | 2 |
Rb3Nd (mp-974850) | 0.0000 | 0.613 | 2 |
Ti3Si (mp-998986) | 0.0000 | 0.194 | 2 |
LiB (mp-1001831) | 0.0000 | 0.386 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ce Au |
Final Energy/Atom-3.9544 eV |
Corrected Energy-15.8176 eV
-15.8176 eV = -15.8176 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)