Final Magnetic Moment4.015 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.355 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density14.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 296.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 111.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 296.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 185.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 321.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 259.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 334.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 52.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 296.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 192.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 262.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 148.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 334.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 185.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 262.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 314.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 148.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 334.0 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 185.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 64.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 334.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 37.1 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 64.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 185.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 148.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 209.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 185.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 259.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 148.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 209.9 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 257.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 185.5 |
Al (mp-134) | <1 0 0> | <1 0 0> | 148.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 209.9 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 1> | 128.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 192.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 111.3 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 185.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 296.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 296.8 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 209.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 209.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 296.8 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 257.1 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 157.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 259.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 222.6 |
BN (mp-984) | <1 1 0> | <1 1 1> | 64.3 |
BN (mp-984) | <1 1 1> | <1 1 0> | 262.4 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 259.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HfInNi2 (mp-640024) | 0.0048 | 0.032 | 3 |
PaInCu2 (mp-862823) | 0.0048 | 0.000 | 3 |
TiInPd2 (mp-866168) | 0.0048 | 0.000 | 3 |
SmInRh2 (mp-867978) | 0.0049 | 0.000 | 3 |
TaInRu2 (mp-867958) | 0.0028 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0082 | 0.000 | 4 |
TiFeCoSi (mp-998971) | 0.0082 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.0082 | 0.028 | 4 |
VFeCoAs (mp-1066006) | 0.0082 | 0.212 | 4 |
VGaFeCo (mp-1066581) | 0.0082 | 0.029 | 4 |
GaFe3 (mp-672661) | 0.0049 | 0.036 | 2 |
Rb3Tc (mp-974820) | 0.0049 | 1.260 | 2 |
Re3F (mp-974458) | 0.0042 | 0.993 | 2 |
TmTe (mp-571233) | 0.0068 | 0.143 | 2 |
EuTe (mp-991027) | 0.0053 | 0.246 | 2 |
Cu (mp-998890) | 0.0082 | 0.037 | 1 |
Kr (mp-974400) | 0.0082 | 0.002 | 1 |
H2 (mp-632250) | 0.0082 | 0.000 | 1 |
Ge (mp-998883) | 0.0082 | 0.339 | 1 |
U (mp-108) | 0.0082 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv Ga_d Ir |
Final Energy/Atom-7.8218 eV |
Corrected Energy-31.2873 eV
-31.2873 eV = -31.2873 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)