Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.069 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.088 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2NiF4 + NiO + NiF2 |
Band Gap2.819 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 254.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 109.2 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 126.1 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 315.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 205.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 145.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 293.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 327.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 181.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 205.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 308.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 145.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 220.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 252.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 327.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 218.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 327.5 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 73.5 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 52.4 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 257.4 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 293.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 145.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 205.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 181.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 262.0 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 315.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 145.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 205.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 262.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 163.9 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 293.8 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 315.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 109.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 163.9 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 319.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 181.9 |
Te2Mo (mp-602) | <1 1 1> | <0 1 1> | 189.1 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 291.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 1> | 189.1 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 245.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 72.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 181.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 254.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 36.4 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 51.5 |
MgO (mp-1265) | <1 1 1> | <0 1 1> | 63.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 181.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 109.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 154.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 252.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co7(SbO6)2 (mp-705595) | 0.1816 | 0.000 | 3 |
Mg2TiO4 (mp-676979) | 0.2254 | 0.006 | 3 |
Zn7(SbO6)2 (mp-675797) | 0.1904 | 0.009 | 3 |
Mg(CuO2)2 (mvc-6517) | 0.2219 | 0.093 | 3 |
Li3FeO3 (mp-770886) | 0.1642 | 0.061 | 3 |
Li2V3SnO8 (mp-774164) | 0.2092 | 0.020 | 4 |
Li2MnV3O8 (mp-775492) | 0.2066 | 0.026 | 4 |
Li2V3FeO8 (mp-775461) | 0.1867 | 0.021 | 4 |
LiMn2OF3 (mp-764789) | 0.2041 | 0.087 | 4 |
LiCo5O3F5 (mp-763930) | 0.1859 | 0.084 | 4 |
Fe3O4 (mp-715491) | 0.2897 | 0.015 | 2 |
Fe3O4 (mp-542433) | 0.3210 | 0.072 | 2 |
Cr3N4 (mp-1014358) | 0.2694 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.2824 | 0.057 | 2 |
Fe3O4 (mp-31770) | 0.3064 | 0.015 | 2 |
Li4Fe3Cu3(SbO8)2 (mp-764385) | 0.2341 | 0.034 | 5 |
Li4Fe3Ni3(SbO8)2 (mp-761969) | 0.2116 | 0.016 | 5 |
Li4Mn3Fe3(SbO8)2 (mp-775013) | 0.2113 | 0.005 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.2351 | 0.040 | 5 |
Li4Fe3Co3(TeO8)2 (mp-849468) | 0.2186 | 0.064 | 5 |
Li3MnFeCo(PO4)3 (mp-764804) | 0.6753 | 0.030 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6641 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6701 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6716 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6730 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O F |
Final Energy/Atom-4.5905 eV |
Corrected Energy-148.6541 eV
-148.6541 eV = -128.5330 eV (uncorrected energy) - 17.3120 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)