material

Hf2MnIr

ID:

mp-865138

DOI:

10.17188/1310429


Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.638 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.97 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 1 1> <1 1 1> 0.001 288.0
C (mp-66) <1 0 0> <1 0 0> 0.001 166.3
Ge (mp-32) <1 0 0> <1 0 0> 0.002 166.3
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.003 176.4
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.003 207.9
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.005 288.0
LiF (mp-1138) <1 0 0> <1 0 0> 0.009 83.1
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.010 176.4
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.015 288.0
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.036 207.9
GaAs (mp-2534) <1 0 0> <1 0 0> 0.041 166.3
Ni (mp-23) <1 0 0> <1 0 0> 0.051 207.9
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.072 117.6
ZnO (mp-2133) <0 0 1> <1 1 1> 0.081 288.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.088 166.3
CsI (mp-614603) <1 1 0> <1 1 0> 0.105 176.4
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.115 144.0
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.145 332.6
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.146 332.6
CdS (mp-672) <1 1 1> <1 0 0> 0.161 207.9
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.174 176.4
Ni (mp-23) <1 1 0> <1 0 0> 0.181 332.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.185 249.4
WS2 (mp-224) <0 0 1> <1 1 0> 0.223 176.4
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.223 176.4
Mg (mp-153) <0 0 1> <1 1 0> 0.252 176.4
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.256 166.3
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.261 288.0
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.284 72.0
KCl (mp-23193) <1 1 1> <1 1 1> 0.302 72.0
KCl (mp-23193) <1 1 0> <1 1 0> 0.306 58.8
KCl (mp-23193) <1 0 0> <1 0 0> 0.319 41.6
GaN (mp-804) <0 0 1> <1 0 0> 0.329 291.0
MgO (mp-1265) <1 1 1> <1 1 1> 0.330 216.0
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.350 176.4
SiC (mp-11714) <1 0 1> <1 0 0> 0.434 291.0
Al (mp-134) <1 0 0> <1 0 0> 0.441 83.1
MgO (mp-1265) <1 1 0> <1 1 0> 0.442 235.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.461 166.3
TbScO3 (mp-31119) <0 1 0> <1 1 0> 0.470 176.4
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.511 207.9
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.520 72.0
AlN (mp-661) <1 0 1> <1 1 0> 0.534 176.4
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.552 235.2
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.568 332.6
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.609 235.2
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.613 288.0
TiO2 (mp-390) <1 0 1> <1 1 0> 0.614 117.6
Cu (mp-30) <1 0 0> <1 0 0> 0.616 166.3
DyScO3 (mp-31120) <0 1 0> <1 1 0> 0.620 176.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
345 122 122 0 -0 -0
122 345 122 0 -0 -0
122 122 345 0 -0 -0
0 0 0 73 -0 -0
-0 -0 -0 -0 73 0
-0 -0 -0 -0 0 73
Compliance Tensor Sij (10-12Pa-1)
3.5 -0.9 -0.9 0 0 0
-0.9 3.5 -0.9 0 0 0
-0.9 -0.9 3.5 0 0 0
0 0 0 13.6 0 0
0 0 0 0 13.6 0
0 0 0 0 0 13.6
Shear Modulus GV
89 GPa
Bulk Modulus KV
196 GPa
Shear Modulus GR
85 GPa
Bulk Modulus KR
196 GPa
Shear Modulus GVRH
87 GPa
Bulk Modulus KVRH
196 GPa
Elastic Anisotropy
0.22
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSbPt (mp-571584) 0.0000 0.080 4
TiFeCoAs (mp-998974) 0.0000 0.146 4
LiMgSbPd (mp-10179) 0.0000 0.067 4
MnGaFeCo (mp-999552) 0.0000 0.045 4
InSb3 (mp-975512) 0.0000 0.243 2
NdAu3 (mp-975073) 0.0000 0.014 2
SmH3 (mp-867857) 0.0000 0.000 2
ScCu3 (mp-973100) 0.0000 0.040 2
Si3P (mp-972741) 0.0000 0.627 2
TiInRh2 (mp-866170) 0.0000 0.000 3
PmInPt2 (mp-862925) 0.0000 0.000 3
Ce2MgAl (mp-984682) 0.0000 0.083 3
Sm2PdRh (mp-972572) 0.0000 0.029 3
Lu2GaCu (mp-973996) 0.0000 0.000 3
Be (mp-20) 0.0000 0.108 1
Nb (mp-75) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.153 1
Br (mp-673171) 0.0000 0.616 1
I (mp-684663) 0.0000 0.455 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Mn_pv Ir
Final Energy/Atom
-10.1213 eV
Corrected Energy
-40.4853 eV
-40.4853 eV = -40.4853 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)