Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.616 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 75.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 308.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 123.4 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 75.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 246.7 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 261.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 226.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 348.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 305.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 305.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 174.5 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 226.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 123.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 174.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 185.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 218.1 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 185.0 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 246.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 218.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 43.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 61.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 218.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 246.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 185.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 348.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 185.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 226.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 305.3 |
BN (mp-984) | <0 0 1> | <1 1 0> | 246.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 218.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 185.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 348.9 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 75.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 302.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 246.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 130.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 246.7 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 308.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 87.2 |
BN (mp-984) | <1 0 1> | <1 1 1> | 226.6 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 43.6 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 246.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 348.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 218.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 185.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 185.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 61.7 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 75.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 43.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 218.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
177 | 116 | 116 | 0 | 0 | 0 |
116 | 177 | 116 | 0 | 0 | 0 |
116 | 116 | 177 | 0 | 0 | 0 |
0 | 0 | 0 | 66 | 0 | 0 |
0 | 0 | 0 | 0 | 66 | 0 |
0 | 0 | 0 | 0 | 0 | 66 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
11.7 | -4.6 | -4.6 | 0 | 0 | 0 |
-4.6 | 11.7 | -4.6 | 0 | 0 | 0 |
-4.6 | -4.6 | 11.7 | 0 | 0 | 0 |
0 | 0 | 0 | 15.2 | 0 | 0 |
0 | 0 | 0 | 0 | 15.2 | 0 |
0 | 0 | 0 | 0 | 0 | 15.2 |
Shear Modulus GV52 GPa |
Bulk Modulus KV136 GPa |
Shear Modulus GR45 GPa |
Bulk Modulus KR136 GPa |
Shear Modulus GVRH48 GPa |
Bulk Modulus KVRH136 GPa |
Elastic Anisotropy0.73 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sc2GaAu (mp-972898) | 0.0000 | 0.007 | 3 |
Sc2GaCu (mp-862340) | 0.0000 | 0.000 | 3 |
ScPaTc2 (mp-862612) | 0.0000 | 0.000 | 3 |
Nd2IrPd (mp-864622) | 0.0000 | 0.033 | 3 |
MgSiRh2 (mp-866087) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.069 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.080 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.067 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
SbPt3 (mp-973353) | 0.0000 | 0.117 | 2 |
Rb3Sn (mp-974789) | 0.0000 | 0.173 | 2 |
LiCd3 (mp-973940) | 0.0000 | 0.015 | 2 |
Rb3Sm (mp-974816) | 0.0000 | 0.656 | 2 |
PmH3 (mp-862910) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.616 | 1 |
Ti (mp-73) | 0.0000 | 0.114 | 1 |
I (mp-684663) | 0.0000 | 0.455 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.153 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Cd Rh_pv |
Final Energy/Atom-5.6429 eV |
Corrected Energy-22.5716 eV
-22.5716 eV = -22.5716 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)