material

TmBr3

ID:

mp-865301

DOI:

10.17188/1310598


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.831 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.95 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.992 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.000 344.5
GaN (mp-804) <0 0 1> <0 0 1> 0.000 279.2
Ni (mp-23) <1 1 1> <0 0 1> 0.001 279.2
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.001 93.1
MgO (mp-1265) <1 1 1> <0 0 1> 0.001 93.1
AlN (mp-661) <1 0 1> <1 0 0> 0.001 229.7
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.001 279.2
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.002 132.6
GaN (mp-804) <1 0 0> <1 0 1> 0.002 100.6
KCl (mp-23193) <1 1 1> <0 0 1> 0.002 279.2
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.002 93.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.002 279.2
MgO (mp-1265) <1 1 0> <1 0 0> 0.003 76.6
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.003 93.1
KCl (mp-23193) <1 1 0> <1 1 1> 0.004 114.3
CdWO4 (mp-19387) <1 1 1> <1 0 0> 0.004 153.1
Ni (mp-23) <1 0 0> <0 0 1> 0.004 186.2
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.004 279.2
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.004 279.2
ZnO (mp-2133) <1 0 0> <0 0 1> 0.004 279.2
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.005 268.0
MgO (mp-1265) <1 0 0> <1 0 0> 0.005 268.0
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.006 229.7
CdS (mp-672) <1 0 0> <1 0 1> 0.006 201.3
Fe2O3 (mp-24972) <1 0 0> <0 0 1> 0.007 279.2
AlN (mp-661) <1 1 0> <1 0 0> 0.008 306.3
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.008 331.5
Au (mp-81) <1 1 1> <0 0 1> 0.008 93.1
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.009 344.5
LiAlO2 (mp-3427) <1 1 1> <1 1 0> 0.009 265.2
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.009 344.5
TiO2 (mp-390) <1 0 1> <1 0 1> 0.009 201.3
C (mp-48) <0 0 1> <1 0 0> 0.010 268.0
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.011 279.2
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.012 93.1
C (mp-48) <1 0 1> <1 0 0> 0.012 306.3
GdScO3 (mp-5690) <0 1 1> <1 0 0> 0.012 268.0
YVO4 (mp-19133) <1 1 0> <1 0 1> 0.013 201.3
C (mp-66) <1 1 0> <1 0 1> 0.014 201.3
CaF2 (mp-2741) <1 1 0> <1 0 0> 0.014 344.5
PbSe (mp-2201) <1 1 1> <0 0 1> 0.014 279.2
AlN (mp-661) <0 0 1> <1 0 0> 0.014 344.5
GaSb (mp-1156) <1 1 1> <0 0 1> 0.016 279.2
PbS (mp-21276) <1 1 0> <1 0 0> 0.016 153.1
LiAlO2 (mp-3427) <0 0 1> <1 1 0> 0.017 132.6
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.017 228.6
Mg (mp-153) <1 1 0> <1 0 0> 0.018 114.8
CdSe (mp-2691) <1 1 1> <0 0 1> 0.018 279.2
BaF2 (mp-1029) <1 1 0> <1 1 1> 0.020 114.3
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.020 344.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
1 0 0 0 0 0
0 1 0 0 0 0
0 0 61 0 0 0
0 0 0 0 0 0
0 0 0 0 0 0
0 0 0 0 0 0
Compliance Tensor Sij (10-12Pa-1)
1370.7 -683.6 -4.1 0 0 0
-683.6 1370.7 -4.1 0 0 0
-4.1 -4.1 16.4 0 0 0
0 0 0 4784.1 0 0
0 0 0 0 4784.1 0
0 0 0 0 0 4108.6
Shear Modulus GV
4 GPa
Bulk Modulus KV
7 GPa
Shear Modulus GR
0 GPa
Bulk Modulus KR
1 GPa
Shear Modulus GVRH
2 GPa
Bulk Modulus KVRH
4 GPa
Elastic Anisotropy
81.81
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
PmI3 (mp-863695) 0.0667 0.000 2
InCl3 (mp-862983) 0.0705 0.000 2
YBr3 (mp-865605) 0.0556 0.061 2
NdI3 (mp-864617) 0.0818 0.000 2
LuBr3 (mp-866214) 0.0753 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Tm_3 Br
Final Energy/Atom
-4.1777 eV
Corrected Energy
-33.4217 eV
-33.4217 eV = -33.4217 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)