Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.727 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.73 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CsI (mp-614603) <1 1 0> <1 1 0> 0.000 261.9
Au (mp-81) <1 1 0> <1 1 0> 0.003 196.4
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.005 80.2
Ag (mp-124) <1 1 0> <1 1 0> 0.006 196.4
GaN (mp-804) <1 1 0> <1 1 0> 0.007 261.9
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.008 324.1
GaN (mp-804) <0 0 1> <1 1 1> 0.020 80.2
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.024 277.8
C (mp-66) <1 0 0> <1 0 0> 0.026 231.5
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.036 160.4
Mg (mp-153) <1 1 0> <1 1 0> 0.039 261.9
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.039 277.8
TiO2 (mp-390) <1 1 0> <1 1 0> 0.050 261.9
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.054 131.0
GaP (mp-2490) <1 1 1> <1 1 0> 0.055 261.9
LiF (mp-1138) <1 1 0> <1 1 0> 0.062 261.9
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.081 160.4
CaF2 (mp-2741) <1 1 1> <1 1 0> 0.084 261.9
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.090 231.5
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.094 327.4
C (mp-66) <1 1 0> <1 1 0> 0.094 196.4
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.095 240.6
BN (mp-984) <1 0 0> <1 0 0> 0.102 231.5
Si (mp-149) <1 1 1> <1 1 0> 0.103 261.9
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.105 231.5
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.106 231.5
CeO2 (mp-20194) <1 1 1> <1 1 0> 0.109 261.9
WS2 (mp-224) <1 0 1> <1 1 0> 0.112 327.4
TiO2 (mp-390) <1 0 0> <1 0 0> 0.120 185.2
BN (mp-984) <0 0 1> <1 0 0> 0.121 231.5
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.135 185.2
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.137 131.0
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.154 277.8
NaCl (mp-22862) <1 1 1> <1 0 0> 0.159 277.8
CdS (mp-672) <1 1 0> <1 1 0> 0.162 196.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.176 185.2
Cu (mp-30) <1 0 0> <1 0 0> 0.176 231.5
Te2W (mp-22693) <0 1 0> <1 0 0> 0.187 324.1
Te2W (mp-22693) <0 1 1> <1 0 0> 0.189 231.5
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.196 231.5
C (mp-48) <0 0 1> <1 0 0> 0.199 324.1
SiC (mp-11714) <1 0 1> <1 0 0> 0.202 324.1
GaP (mp-2490) <1 1 0> <1 1 0> 0.212 131.0
NdGaO3 (mp-3196) <0 1 1> <1 1 1> 0.217 160.4
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.223 261.9
ZnO (mp-2133) <1 0 0> <1 1 0> 0.280 261.9
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.283 327.4
GaSe (mp-1943) <0 0 1> <1 0 0> 0.284 231.5
MgO (mp-1265) <1 0 0> <1 0 0> 0.294 92.6
InP (mp-20351) <1 1 0> <1 1 0> 0.318 196.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
111 91 91 0 0 0
91 111 91 0 0 0
91 91 111 0 0 0
0 0 0 41 0 0
0 0 0 0 41 0
0 0 0 0 0 41
Compliance Tensor Sij (10-12Pa-1)
35.7 -16.2 -16.2 0 0 0
-16.2 35.7 -16.2 0 0 0
-16.2 -16.2 35.7 0 0 0
0 0 0 24.2 0 0
0 0 0 0 24.2 0
0 0 0 0 0 24.2
Shear Modulus GV
29 GPa
Bulk Modulus KV
98 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
98 GPa
Shear Modulus GVRH
23 GPa
Bulk Modulus KVRH
98 GPa
Elastic Anisotropy
3.03
Poisson's Ratio
0.39

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nd2ZnIr (mp-977445) 0.0000 0.056 3
LiEr2Ir (mp-862554) 0.0000 0.000 3
Pm2CuGe (mp-863664) 0.0000 0.000 3
Dy2CuOs (mp-864959) 0.0000 0.000 3
SrMgTl2 (mp-867172) 0.0000 0.000 3
TiFeCoAs (mp-998974) 0.0000 0.146 4
TiGaFeCo (mp-998964) 0.0000 0.000 4
TiFeCoSb (mp-998973) 0.0000 0.198 4
TiAlFeCo (mp-998980) 0.0000 0.000 4
MnFeCoGe (mp-1018024) 0.0000 0.009 4
K3Zr (mp-973265) 0.0000 0.979 2
Sb3Mo (mp-973203) 0.0000 0.613 2
SiBi3 (mp-972837) 0.0000 0.436 2
RePb3 (mp-974611) 0.0000 1.028 2
PrW3 (mp-975787) 0.0000 0.792 2
Xe (mp-979285) 0.0000 0.002 1
Cu (mp-998890) 0.0000 0.035 1
Kr (mp-974400) 0.0000 0.002 1
H2 (mp-632250) 0.0000 0.000 1
Ge (mp-998883) 0.0000 0.346 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Cd Pd
Final Energy/Atom
-5.1639 eV
Corrected Energy
-20.6555 eV
-20.6555 eV = -20.6555 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)