Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.407 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 155.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 73.4 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 89.9 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 259.5 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 207.6 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 220.2 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 269.7 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 259.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 259.5 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 259.5 |
Au (mp-81) | <1 1 0> | <1 1 0> | 73.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 207.6 |
Au (mp-81) | <1 1 1> | <1 1 1> | 89.9 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 220.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 51.9 |
GaSb (mp-1156) | <1 1 1> | <1 1 1> | 269.7 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 220.2 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 207.6 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 51.9 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 293.6 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 73.4 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 89.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 220.2 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 269.7 |
GaTe (mp-542812) | <1 0 1> | <1 1 0> | 293.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 259.5 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 220.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 220.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 220.2 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 220.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 207.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 220.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 51.9 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 220.2 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 269.7 |
C (mp-66) | <1 1 0> | <1 1 0> | 73.4 |
C (mp-66) | <1 1 1> | <1 1 1> | 89.9 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 220.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 259.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 207.6 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 89.9 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 220.2 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 220.2 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 89.9 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 269.7 |
BN (mp-984) | <1 1 0> | <1 1 1> | 269.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 155.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 220.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 259.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 220.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
95 | 46 | 46 | 0 | 0 | 0 |
46 | 95 | 46 | 0 | 0 | 0 |
46 | 46 | 95 | 0 | 0 | 0 |
0 | 0 | 0 | 58 | 0 | 0 |
0 | 0 | 0 | 0 | 58 | 0 |
0 | 0 | 0 | 0 | 0 | 58 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
15.7 | -5.2 | -5.2 | 0 | 0 | 0 |
-5.2 | 15.7 | -5.2 | 0 | 0 | 0 |
-5.2 | -5.2 | 15.7 | 0 | 0 | 0 |
0 | 0 | 0 | 17.3 | 0 | 0 |
0 | 0 | 0 | 0 | 17.3 | 0 |
0 | 0 | 0 | 0 | 0 | 17.3 |
Shear Modulus GV44 GPa |
Bulk Modulus KV63 GPa |
Shear Modulus GR37 GPa |
Bulk Modulus KR63 GPa |
Shear Modulus GVRH41 GPa |
Bulk Modulus KVRH63 GPa |
Elastic Anisotropy0.98 |
Poisson's Ratio0.23 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoErTl2 (mp-974221) | 0.0000 | 0.000 | 3 |
AcHgAu2 (mp-861966) | 0.0000 | 0.000 | 3 |
PaCdAu2 (mp-861973) | 0.0000 | 0.000 | 3 |
TiSiOs2 (mp-865680) | 0.0000 | 0.000 | 3 |
BeSiRh2 (mp-867767) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Yb3Mn (mp-979955) | 0.0000 | 0.315 | 2 |
InSb3 (mp-975512) | 0.0000 | 0.245 | 2 |
LiCd3 (mp-973940) | 0.0000 | 0.000 | 2 |
Li3Ge (mp-867342) | 0.0000 | 0.007 | 2 |
Rb3Pr (mp-974828) | 0.0000 | 0.608 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Al Zn |
Final Energy/Atom-4.8911 eV |
Corrected Energy-19.5644 eV
-19.5644 eV = -19.5644 eV (uncorrected energy)
|