Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.613 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 1> | 276.7 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 225.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 266.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 225.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 150.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 266.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 266.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 213.0 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 150.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 213.0 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 225.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 53.2 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 225.9 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 213.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 213.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 266.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 225.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 266.2 |
BN (mp-984) | <1 1 0> | <1 1 1> | 276.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 213.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 266.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 92.2 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 75.3 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 92.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 106.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 319.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 266.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 159.7 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 225.9 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 53.2 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 150.6 |
PbS (mp-21276) | <1 1 1> | <1 1 0> | 301.2 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 150.6 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 266.2 |
Ni (mp-23) | <1 0 0> | <1 1 1> | 184.4 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 213.0 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 225.9 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 276.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 213.0 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 266.2 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 225.9 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 225.9 |
Au (mp-81) | <1 1 0> | <1 1 0> | 75.3 |
Au (mp-81) | <1 1 1> | <1 1 1> | 92.2 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 225.9 |
C (mp-48) | <1 1 0> | <1 1 0> | 301.2 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 225.9 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 150.6 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 266.2 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 159.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
81 | 69 | 69 | 0 | 0 | 0 |
69 | 81 | 69 | 0 | 0 | 0 |
69 | 69 | 81 | 0 | 0 | 0 |
0 | 0 | 0 | 34 | 0 | 0 |
0 | 0 | 0 | 0 | 34 | 0 |
0 | 0 | 0 | 0 | 0 | 34 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
60.2 | -27.8 | -27.8 | 0 | 0 | 0 |
-27.8 | 60.2 | -27.8 | 0 | 0 | 0 |
-27.8 | -27.8 | 60.2 | 0 | 0 | 0 |
0 | 0 | 0 | 29.3 | 0 | 0 |
0 | 0 | 0 | 0 | 29.3 | 0 |
0 | 0 | 0 | 0 | 0 | 29.3 |
Shear Modulus GV23 GPa |
Bulk Modulus KV73 GPa |
Shear Modulus GR11 GPa |
Bulk Modulus KR73 GPa |
Shear Modulus GVRH17 GPa |
Bulk Modulus KVRH73 GPa |
Elastic Anisotropy5.00 |
Poisson's Ratio0.39 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTmZn2 (mp-983126) | 0.0000 | 0.000 | 3 |
Pm2PtAu (mp-982772) | 0.0000 | 0.000 | 3 |
Nd2IrAu (mp-973606) | 0.0000 | 0.057 | 3 |
YbPrPd2 (mp-981530) | 0.0000 | 0.011 | 3 |
YTmAl2 (mp-980662) | 0.0000 | 0.016 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.163 | 4 |
ErPd (mp-851) | 0.0000 | 0.000 | 2 |
YbRu (mp-567116) | 0.0000 | 0.209 | 2 |
PrIn (mp-20023) | 0.0000 | 0.000 | 2 |
ReC (mp-1009731) | 0.0000 | 1.115 | 2 |
ScCu (mp-1169) | 0.0000 | 0.000 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Pb_d Au |
Final Energy/Atom-4.3703 eV |
Corrected Energy-17.4813 eV
-17.4813 eV = -17.4813 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)