material

GaCu3

ID:

mp-865798

DOI:

10.17188/1310997


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.093 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.002 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.65 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
GaCu3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 1 1> <0 0 1> 0.000 70.8
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.000 23.6
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.003 154.7
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.003 221.0
BN (mp-984) <0 0 1> <0 0 1> 0.006 70.8
MgO (mp-1265) <1 1 1> <0 0 1> 0.006 94.5
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.008 66.3
AlN (mp-661) <1 0 1> <1 1 0> 0.008 267.9
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.010 191.4
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.011 110.5
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.013 344.4
PbS (mp-21276) <1 1 0> <1 1 0> 0.014 153.1
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.015 23.6
LiAlO2 (mp-3427) <1 0 1> <1 0 1> 0.020 129.4
GaP (mp-2490) <1 1 0> <1 1 0> 0.021 344.4
MgO (mp-1265) <1 1 0> <1 1 0> 0.026 76.5
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.028 118.1
InSb (mp-20012) <1 1 1> <0 0 1> 0.028 307.0
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.028 94.5
SiC (mp-8062) <1 1 0> <1 0 1> 0.031 161.7
GaSe (mp-1943) <0 0 1> <0 0 1> 0.031 165.3
CdTe (mp-406) <1 1 1> <0 0 1> 0.039 307.0
Mg (mp-153) <1 0 0> <1 0 0> 0.041 66.3
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.041 154.7
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.043 307.0
InP (mp-20351) <1 1 1> <1 1 0> 0.045 306.2
InP (mp-20351) <1 0 0> <1 0 0> 0.045 176.8
Mg (mp-153) <0 0 1> <0 0 1> 0.047 165.3
KCl (mp-23193) <1 1 0> <1 1 0> 0.050 114.8
CdS (mp-672) <0 0 1> <1 0 0> 0.050 154.7
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.059 307.0
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.066 212.5
Te2W (mp-22693) <1 0 1> <1 0 0> 0.068 198.9
GaN (mp-804) <1 0 1> <1 0 0> 0.069 132.6
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.070 344.4
C (mp-48) <1 1 0> <1 0 0> 0.072 66.3
ZrO2 (mp-2858) <1 0 1> <1 0 1> 0.076 129.4
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.078 176.8
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.078 134.9
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.079 134.9
BaTiO3 (mp-5986) <0 0 1> <1 1 1> 0.087 269.8
C (mp-48) <0 0 1> <1 1 0> 0.087 114.8
Al (mp-134) <1 1 1> <1 1 1> 0.089 314.8
AlN (mp-661) <1 1 1> <1 0 1> 0.090 258.7
TiO2 (mp-390) <1 1 0> <1 0 1> 0.091 258.7
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.097 110.5
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.097 161.7
LaF3 (mp-905) <0 0 1> <1 0 1> 0.099 226.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.104 165.3
WS2 (mp-224) <0 0 1> <0 0 1> 0.105 165.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
188 109 82 0 0 0
109 188 82 0 0 0
82 82 220 0 0 0
0 0 0 45 0 0
0 0 0 0 45 0
0 0 0 0 0 40
Compliance Tensor Sij (10-12Pa-1)
8.4 -4.2 -1.6 0 0 0
-4.2 8.4 -1.6 0 0 0
-1.6 -1.6 5.7 0 0 0
0 0 0 22.3 0 0
0 0 0 0 22.3 0
0 0 0 0 0 25.3
Shear Modulus GV
47 GPa
Bulk Modulus KV
127 GPa
Shear Modulus GR
46 GPa
Bulk Modulus KR
127 GPa
Shear Modulus GVRH
47 GPa
Bulk Modulus KVRH
127 GPa
Elastic Anisotropy
0.21
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NaCaMg6 (mp-1099110) 0.0197 0.111 3
Cr8Ni50Mo15W2 (mp-767372) 0.2572 0.028 4
CrFeCoNi (mp-1012640) 0.1875 0.065 4
CrFeCoNi (mp-1096923) 0.3935 0.193 4
NaCd3 (mp-973166) 0.0089 0.016 2
LaNd3 (mp-977225) 0.0123 0.034 2
K3Rb (mp-976115) 0.0075 0.022 2
Cs3Rb (mp-862689) 0.0106 0.056 2
Hf3Mg (mp-1094259) 0.0134 0.107 2
Co (mp-987206) 0.0273 0.000 1
Co (mp-54) 0.0274 0.000 1
Tl (mp-82) 0.0281 0.004 1
Na (mp-10172) 0.0274 0.010 1
Cs (mp-11832) 0.0274 0.035 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ga_d Cu_pv
Final Energy/Atom
-3.9244 eV
Corrected Energy
-31.3955 eV
Uncorrected energy = -31.3955 eV Corrected energy = -31.3955 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)