material

Ti2RuOs

ID:

mp-865842

DOI:

10.17188/1311028


Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.742 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.88 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiOs + TiRu
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 1 1> <1 1 1> 0.000 66.2
InAs (mp-20305) <1 1 0> <1 1 0> 0.000 54.1
InAs (mp-20305) <1 0 0> <1 0 0> 0.000 38.2
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.000 66.2
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.000 54.1
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.000 38.2
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.003 66.2
TePb (mp-19717) <1 0 0> <1 0 0> 0.008 344.1
C (mp-66) <1 1 1> <1 1 1> 0.009 66.2
C (mp-66) <1 1 0> <1 1 0> 0.009 54.1
CdS (mp-672) <0 0 1> <1 1 1> 0.010 198.6
SiC (mp-7631) <1 0 1> <1 0 0> 0.012 191.1
SiC (mp-8062) <1 1 0> <1 1 0> 0.015 54.1
SiC (mp-8062) <1 0 0> <1 0 0> 0.015 38.2
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.016 305.8
SiC (mp-7631) <1 1 0> <1 1 0> 0.018 162.2
Te2Mo (mp-602) <1 1 1> <1 0 0> 0.022 191.1
Al (mp-134) <1 1 1> <1 1 1> 0.023 198.6
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.023 198.6
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.034 152.9
Ni (mp-23) <1 0 0> <1 0 0> 0.046 305.8
MgO (mp-1265) <1 0 0> <1 0 0> 0.065 305.8
AlN (mp-661) <0 0 1> <1 1 1> 0.076 264.9
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.085 198.6
Mg (mp-153) <0 0 1> <1 0 0> 0.089 305.8
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.091 198.6
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.092 162.2
GaP (mp-2490) <1 0 0> <1 0 0> 0.097 152.9
ZnO (mp-2133) <0 0 1> <1 1 1> 0.112 66.2
CdSe (mp-2691) <1 1 1> <1 1 1> 0.115 66.2
CdSe (mp-2691) <1 1 0> <1 1 0> 0.116 54.1
C (mp-66) <1 0 0> <1 1 0> 0.119 270.3
CdSe (mp-2691) <1 0 0> <1 0 0> 0.122 38.2
CsI (mp-614603) <1 0 0> <1 0 0> 0.125 305.8
GaN (mp-804) <1 1 0> <1 1 0> 0.129 324.4
SiC (mp-8062) <1 1 1> <1 0 0> 0.136 267.6
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.149 191.1
GaN (mp-804) <1 1 1> <1 0 0> 0.151 152.9
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.156 66.2
SiC (mp-7631) <0 0 1> <1 0 0> 0.160 267.6
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.167 305.8
GaSb (mp-1156) <1 1 1> <1 1 1> 0.168 66.2
WS2 (mp-224) <0 0 1> <1 0 0> 0.168 305.8
GaSb (mp-1156) <1 1 0> <1 1 0> 0.170 54.1
Mg (mp-153) <1 1 1> <1 0 0> 0.171 152.9
SiC (mp-11714) <0 0 1> <1 0 0> 0.172 267.6
GaSb (mp-1156) <1 0 0> <1 0 0> 0.179 38.2
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.194 344.1
WSe2 (mp-1821) <1 1 1> <1 1 1> 0.217 264.9
GaN (mp-804) <1 0 1> <1 1 0> 0.229 270.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
440 127 127 0 0 0
127 440 127 0 0 0
127 127 440 0 0 0
0 0 0 103 0 0
0 0 0 0 103 0
0 0 0 0 0 103
Compliance Tensor Sij (10-12Pa-1)
2.6 -0.6 -0.6 0 0 0
-0.6 2.6 -0.6 0 0 0
-0.6 -0.6 2.6 0 0 0
0 0 0 9.7 0 0
0 0 0 0 9.7 0
0 0 0 0 0 9.7
Shear Modulus GV
125 GPa
Bulk Modulus KV
231 GPa
Shear Modulus GR
120 GPa
Bulk Modulus KR
231 GPa
Shear Modulus GVRH
122 GPa
Bulk Modulus KVRH
231 GPa
Elastic Anisotropy
0.21
Poisson's Ratio
0.28

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
28
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Os_pv Ru_pv
Final Energy/Atom
-9.8122 eV
Corrected Energy
-39.2487 eV
-39.2487 eV = -39.2487 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)