Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.404 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 168.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 278.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 281.5 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 168.9 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 206.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 159.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 39.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 56.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 69.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 275.8 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 168.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 159.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 199.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 238.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 39.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 56.3 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 69.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 337.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 318.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 39.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 56.3 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 69.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 159.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 79.6 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 225.2 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 206.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 112.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 275.8 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 199.0 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 199.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 199.0 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 225.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 199.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 358.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 199.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 275.8 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 275.8 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 199.0 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 199.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 159.2 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 225.2 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 206.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 69.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 199.0 |
BN (mp-984) | <1 0 1> | <1 1 0> | 337.8 |
BN (mp-984) | <1 1 0> | <1 1 1> | 69.0 |
BN (mp-984) | <1 1 1> | <1 0 0> | 278.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 69.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 225.2 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 275.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
62 | 52 | 52 | 0 | 0 | 0 |
52 | 62 | 52 | 0 | 0 | 0 |
52 | 52 | 62 | 0 | 0 | 0 |
0 | 0 | 0 | 30 | 0 | 0 |
0 | 0 | 0 | 0 | 30 | 0 |
0 | 0 | 0 | 0 | 0 | 30 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
65.6 | -29.8 | -29.8 | 0 | 0 | 0 |
-29.8 | 65.6 | -29.8 | 0 | 0 | 0 |
-29.8 | -29.8 | 65.6 | 0 | 0 | 0 |
0 | 0 | 0 | 33.7 | 0 | 0 |
0 | 0 | 0 | 0 | 33.7 | 0 |
0 | 0 | 0 | 0 | 0 | 33.7 |
Shear Modulus GV20 GPa |
Bulk Modulus KV55 GPa |
Shear Modulus GR10 GPa |
Bulk Modulus KR55 GPa |
Shear Modulus GVRH15 GPa |
Bulk Modulus KVRH55 GPa |
Elastic Anisotropy4.60 |
Poisson's Ratio0.37 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NdCdAu2 (mp-977562) | 0.0000 | 0.000 | 3 |
ErCdAg2 (mp-977378) | 0.0000 | 0.000 | 3 |
La2MgTl (mp-977187) | 0.0000 | 0.011 | 3 |
TmHfOs2 (mp-865209) | 0.0000 | 0.094 | 3 |
YZrRu2 (mp-866159) | 0.0000 | 0.024 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Yb3Mn (mp-979955) | 0.0000 | 0.315 | 2 |
K3Tl (mp-974641) | 0.0000 | 0.075 | 2 |
Li3Nd (mp-976264) | 0.0000 | 0.197 | 2 |
K3Sn (mp-973614) | 0.0000 | 0.105 | 2 |
Rb3Pr (mp-974828) | 0.0000 | 0.608 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ag Au |
Final Energy/Atom-2.8851 eV |
Corrected Energy-11.5406 eV
-11.5406 eV = -11.5406 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)