Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.250 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 305.4 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 229.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 269.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 269.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 229.0 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 280.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 269.9 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 229.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 280.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 305.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 305.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 152.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 215.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 229.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 280.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 269.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 229.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 280.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 269.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 215.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 152.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 215.9 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 229.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 54.0 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 229.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 215.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 323.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 215.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 269.9 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 93.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 269.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 215.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 269.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 269.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 93.5 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 108.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 215.9 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 269.9 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 269.9 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 305.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 1 0> | 229.0 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 269.9 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 54.0 |
PbS (mp-21276) | <1 1 1> | <1 1 0> | 305.4 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 269.9 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 152.7 |
InP (mp-20351) | <1 1 1> | <1 1 0> | 305.4 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 269.9 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 215.9 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 229.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
61 | 19 | 19 | -0 | 0 | 0 |
19 | 61 | 19 | -0 | 0 | 0 |
19 | 19 | 61 | -0 | 0 | 0 |
-0 | -0 | -0 | 15 | 0 | 0 |
0 | 0 | 0 | 0 | 15 | -0 |
0 | 0 | 0 | 0 | -0 | 15 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
19.1 | -4.5 | -4.5 | 0 | 0 | 0 |
-4.5 | 19.1 | -4.5 | 0 | 0 | 0 |
-4.5 | -4.5 | 19.1 | 0 | 0 | 0 |
0 | 0 | 0 | 68.6 | -0.1 | -0.1 |
0 | 0 | 0 | -0.1 | 68.6 | 0.1 |
0 | 0 | 0 | -0.1 | 0.1 | 68.6 |
Shear Modulus GV17 GPa |
Bulk Modulus KV33 GPa |
Shear Modulus GR17 GPa |
Bulk Modulus KR33 GPa |
Shear Modulus GVRH17 GPa |
Bulk Modulus KVRH33 GPa |
Elastic Anisotropy0.17 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NdZn2Ag (mp-974744) | 0.0037 | 0.024 | 3 |
LiZrIr2 (mp-865925) | 0.0027 | 0.000 | 3 |
TmNbOs2 (mp-865241) | 0.0052 | 0.083 | 3 |
CaSmZn2 (mp-866061) | 0.0022 | 0.000 | 3 |
AlSiRu2 (mp-862778) | 0.0042 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0140 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0140 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0140 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0140 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0140 | 0.000 | 4 |
GeTe (mp-672698) | 0.0103 | 0.326 | 2 |
GaFe3 (mp-672661) | 0.0131 | 0.036 | 2 |
Rb3Tc (mp-974820) | 0.0131 | 1.248 | 2 |
TmTe (mp-571233) | 0.0131 | 0.143 | 2 |
PmAg3 (mp-862878) | 0.0123 | 0.000 | 2 |
Br (mp-673171) | 0.0140 | 0.630 | 1 |
Ti (mp-73) | 0.0140 | 0.112 | 1 |
I (mp-684663) | 0.0140 | 0.446 | 1 |
Cr (mp-90) | 0.0140 | 0.000 | 1 |
Bi (mp-568610) | 0.0140 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ac In_d |
Final Energy/Atom-2.9230 eV |
Corrected Energy-11.6918 eV
-11.6918 eV = -11.6918 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)