Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.669 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKNd(SO4)2 |
Band Gap5.449 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 246.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 190.9 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 293.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 291.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 191.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 349.1 |
SiO2 (mp-6930) | <1 1 1> | <1 -1 1> | 261.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 259.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 255.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 255.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 255.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 218.9 |
Te2W (mp-22693) | <0 1 1> | <1 1 -1> | 172.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 199.5 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 172.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 -1> | 175.9 |
BN (mp-984) | <1 0 1> | <0 1 1> | 200.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 305.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 319.8 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 267.2 |
Al (mp-134) | <1 0 0> | <1 1 -1> | 259.0 |
Al (mp-134) | <1 1 0> | <1 0 0> | 255.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 283.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 303.8 |
SiC (mp-7631) | <0 0 1> | <1 -1 0> | 240.6 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 229.1 |
SiC (mp-7631) | <1 1 0> | <0 1 -1> | 234.5 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 303.8 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 149.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 319.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 249.4 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 293.2 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 151.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 152.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 283.2 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 291.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 149.6 |
YVO4 (mp-19133) | <0 0 1> | <1 -1 -1> | 271.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 267.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 218.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 229.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 200.2 |
BN (mp-984) | <0 0 1> | <1 -1 1> | 87.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 267.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 303.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 -1> | 293.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 229.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 -1> | 293.2 |
MgO (mp-1265) | <1 0 0> | <0 1 -1> | 234.5 |
MgO (mp-1265) | <1 1 0> | <1 -1 -1> | 180.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs2MnO4 (mp-775233) | 0.4435 | 0.030 | 3 |
Ce(SO4)2 (mp-21947) | 0.4695 | 0.000 | 3 |
Tl2SeO4 (mp-559961) | 0.3921 | 0.000 | 3 |
CrPbO4 (mp-19146) | 0.4042 | 0.000 | 3 |
NaClO4 (mp-22968) | 0.4747 | 0.000 | 3 |
KEr(SO4)2 (mp-18555) | 0.3921 | 0.007 | 4 |
KPr(SO4)2 (mp-554057) | 0.2740 | 0.000 | 4 |
Na2Th(PO4)2 (mp-582483) | 0.4198 | 0.000 | 4 |
Na2Th(PO4)2 (mp-555861) | 0.4253 | 0.001 | 4 |
SrTlVO4 (mp-566556) | 0.4300 | 0.000 | 4 |
GaBr2 (mp-650841) | 0.5744 | 0.011 | 2 |
GaCl2 (mp-568848) | 0.7453 | 0.000 | 2 |
SiI2 (mp-541053) | 0.7388 | 0.026 | 2 |
KBiS(ClO2)2 (mp-23645) | 0.4520 | 0.000 | 5 |
RbHoHS2O9 (mp-761809) | 0.3418 | 0.080 | 5 |
K2YbMoPO8 (mp-565817) | 0.5379 | 0.003 | 5 |
K2BiMoPO8 (mp-566924) | 0.5436 | 0.000 | 5 |
K2BiPWO8 (mp-566769) | 0.5426 | 0.001 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Nd_3 S O |
Final Energy/Atom-6.5683 eV |
Corrected Energy-171.5289 eV
-171.5289 eV = -157.6384 eV (uncorrected energy) - 13.8905 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)