Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.414 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 227.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 227.5 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 227.5 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 284.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 197.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 295.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 262.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 32.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 46.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 56.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 164.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 164.2 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 232.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 262.7 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 139.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 164.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 92.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 131.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 278.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 46.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 164.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 65.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 295.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 32.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 46.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 56.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 32.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 46.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 229.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 328.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 325.1 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 227.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 262.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 32.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 46.4 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 229.9 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 278.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 262.7 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 139.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 164.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 185.8 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 227.5 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 227.5 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 170.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 164.2 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 229.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 227.5 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 185.8 |
BN (mp-984) | <0 0 1> | <1 1 1> | 170.6 |
BN (mp-984) | <1 0 1> | <1 1 0> | 185.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
167 | 146 | 146 | 0 | 0 | 0 |
146 | 167 | 146 | 0 | 0 | 0 |
146 | 146 | 167 | 0 | 0 | 0 |
0 | 0 | 0 | 71 | 0 | 0 |
0 | 0 | 0 | 0 | 71 | 0 |
0 | 0 | 0 | 0 | 0 | 71 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
31.6 | -14.7 | -14.7 | 0 | 0 | 0 |
-14.7 | 31.6 | -14.7 | 0 | 0 | 0 |
-14.7 | -14.7 | 31.6 | 0 | 0 | 0 |
0 | 0 | 0 | 14 | 0 | 0 |
0 | 0 | 0 | 0 | 14 | 0 |
0 | 0 | 0 | 0 | 0 | 14 |
Shear Modulus GV47 GPa |
Bulk Modulus KV153 GPa |
Shear Modulus GR22 GPa |
Bulk Modulus KR153 GPa |
Shear Modulus GVRH35 GPa |
Bulk Modulus KVRH153 GPa |
Elastic Anisotropy5.71 |
Poisson's Ratio0.40 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TmLuHg2 (mp-972478) | 0.0000 | 0.006 | 3 |
LaOs2Rh (mp-631522) | 0.0000 | 1.127 | 3 |
GaFe2Ni (mp-622990) | 0.0000 | 0.188 | 3 |
HfInCo2 (mp-864715) | 0.0000 | 0.000 | 3 |
CeTlAu2 (mp-867361) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
FeAu3 (mp-973557) | 0.0000 | 0.154 | 2 |
Nb3Ru (mp-977434) | 0.0000 | 0.000 | 2 |
LiCu3 (mp-974058) | 0.0000 | 0.017 | 2 |
Pa3Tc (mp-973853) | 0.0000 | 0.124 | 2 |
Li3Cd (mp-867343) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Be_sv Rh_pv Au |
Final Energy/Atom-4.9437 eV |
Corrected Energy-19.7749 eV
-19.7749 eV = -19.7749 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)