material

TiAlRu2

ID:

mp-866155

DOI:

10.17188/1311409


Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.765 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.11 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaAs (mp-2534) <1 0 0> <1 0 0> 0.000 297.5
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.004 193.3
SiC (mp-7631) <0 0 1> <1 1 1> 0.004 257.7
C (mp-48) <0 0 1> <1 1 1> 0.007 257.7
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.007 297.5
SiC (mp-11714) <0 0 1> <1 1 1> 0.007 257.7
Cu (mp-30) <1 1 0> <1 1 0> 0.014 315.6
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.021 257.7
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.021 257.7
Ge (mp-32) <1 0 0> <1 0 0> 0.022 297.5
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.023 148.8
Si (mp-149) <1 0 0> <1 0 0> 0.028 148.8
Au (mp-81) <1 0 0> <1 0 0> 0.036 297.5
AlN (mp-661) <0 0 1> <1 0 0> 0.049 297.5
Ni (mp-23) <1 1 0> <1 1 0> 0.057 52.6
Ni (mp-23) <1 1 1> <1 1 1> 0.057 64.4
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.060 223.2
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.070 210.4
LiF (mp-1138) <1 0 0> <1 0 0> 0.080 148.8
LiF (mp-1138) <1 1 0> <1 1 0> 0.081 210.4
LiF (mp-1138) <1 1 1> <1 1 1> 0.081 257.7
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.082 257.7
BN (mp-984) <0 0 1> <1 0 0> 0.109 260.3
Mg (mp-153) <1 1 0> <1 1 0> 0.124 315.6
Ag (mp-124) <1 0 0> <1 0 0> 0.125 297.5
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.134 260.3
LaF3 (mp-905) <1 0 0> <1 1 1> 0.140 322.1
GaN (mp-804) <1 0 0> <1 0 0> 0.143 186.0
WSe2 (mp-1821) <1 1 0> <1 1 1> 0.145 257.7
ZnO (mp-2133) <0 0 1> <1 1 0> 0.157 263.0
Al (mp-134) <1 0 0> <1 0 0> 0.179 148.8
Al (mp-134) <1 1 0> <1 1 0> 0.182 210.4
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.183 297.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.192 157.8
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.225 157.8
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.233 223.2
SiC (mp-11714) <1 0 0> <1 0 0> 0.248 186.0
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.249 260.3
SiC (mp-7631) <1 0 0> <1 0 0> 0.254 186.0
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.278 315.6
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.279 210.4
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.280 64.4
Mg (mp-153) <1 1 1> <1 0 0> 0.301 148.8
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.303 148.8
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.307 210.4
ZrO2 (mp-2858) <0 1 1> <1 1 1> 0.311 193.3
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.320 186.0
GaN (mp-804) <1 1 0> <1 1 0> 0.324 315.6
CaCO3 (mp-3953) <1 0 0> <1 1 1> 0.324 257.7
CaCO3 (mp-3953) <1 1 0> <1 0 0> 0.325 148.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
315 156 156 0 0 0
156 315 156 0 0 0
156 156 315 0 0 0
0 0 0 91 0 0
0 0 0 0 91 0
0 0 0 0 0 91
Compliance Tensor Sij (10-12Pa-1)
4.7 -1.6 -1.6 0 0 0
-1.6 4.7 -1.6 0 0 0
-1.6 -1.6 4.7 0 0 0
0 0 0 11 0 0
0 0 0 0 11 0
0 0 0 0 0 11
Shear Modulus GV
87 GPa
Bulk Modulus KV
209 GPa
Shear Modulus GR
86 GPa
Bulk Modulus KR
209 GPa
Shear Modulus GVRH
86 GPa
Bulk Modulus KVRH
209 GPa
Elastic Anisotropy
0.02
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
La2PdRu (mp-973099) 0.0000 0.068 3
Dy2InHg (mp-984660) 0.0000 0.003 3
Hf2ReIr (mp-861978) 0.0000 0.000 3
La2CuIr (mp-862536) 0.0000 0.071 3
SmMgAg2 (mp-867862) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
LiMgSbPt (mp-571584) 0.0000 0.086 4
LiMgSbPd (mp-10179) 0.0000 0.074 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
K3Cd (mp-983062) 0.0000 0.057 2
K3Sc (mp-973535) 0.0000 0.615 2
Ag3Ge (mp-985283) 0.0000 0.100 2
Li3Zn (mp-976412) 0.0000 0.006 2
PmCd3 (mp-862899) 0.0000 0.000 2
Br (mp-673171) 0.0000 0.630 1
Ti (mp-73) 0.0000 0.112 1
I (mp-684663) 0.0000 0.446 1
Cr (mp-90) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.139 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Al Ru_pv
Final Energy/Atom
-8.3129 eV
Corrected Energy
-33.2518 eV
-33.2518 eV = -33.2518 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by