material

YMgHg2

ID:

mp-866164

DOI:

10.17188/1311418


Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.465 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.15 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 0 0> <1 0 0> 0.000 259.3
Ag (mp-124) <1 1 0> <1 1 0> 0.001 73.3
Ag (mp-124) <1 1 1> <1 1 1> 0.001 89.8
PbSe (mp-2201) <1 1 0> <1 1 0> 0.005 220.0
PbSe (mp-2201) <1 1 1> <1 1 1> 0.005 269.5
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.006 259.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.007 207.4
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.007 259.3
TiO2 (mp-390) <0 0 1> <1 0 0> 0.015 259.3
SiC (mp-11714) <1 0 0> <1 1 0> 0.016 220.0
GaSb (mp-1156) <1 1 0> <1 1 0> 0.017 220.0
GaSb (mp-1156) <1 1 1> <1 1 1> 0.017 269.5
Au (mp-81) <1 1 0> <1 1 0> 0.022 73.3
Au (mp-81) <1 1 1> <1 1 1> 0.023 89.8
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.024 207.4
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.027 51.9
CdSe (mp-2691) <1 1 0> <1 1 0> 0.030 220.0
CdSe (mp-2691) <1 1 1> <1 1 1> 0.031 269.5
GaTe (mp-542812) <1 0 1> <1 1 0> 0.034 293.4
Ni (mp-23) <1 0 0> <1 0 0> 0.035 207.4
Cu (mp-30) <1 0 0> <1 0 0> 0.037 51.9
Ni (mp-23) <1 1 0> <1 1 0> 0.038 293.4
Cu (mp-30) <1 1 0> <1 1 0> 0.040 73.3
Cu (mp-30) <1 1 1> <1 1 1> 0.041 89.8
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.052 259.3
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.054 220.0
Te2Mo (mp-602) <0 0 1> <1 1 0> 0.058 220.0
SiC (mp-11714) <1 1 0> <1 1 0> 0.091 220.0
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.091 220.0
KCl (mp-23193) <1 0 0> <1 0 0> 0.098 207.4
SiC (mp-8062) <1 1 0> <1 1 0> 0.099 220.0
C (mp-66) <1 0 0> <1 0 0> 0.102 51.9
BN (mp-984) <1 1 0> <1 1 1> 0.107 269.5
C (mp-66) <1 1 0> <1 1 0> 0.110 73.3
C (mp-66) <1 1 1> <1 1 1> 0.112 89.8
BN (mp-984) <0 0 1> <1 1 0> 0.114 220.0
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.118 220.0
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.120 269.5
AlN (mp-661) <1 1 0> <1 1 0> 0.128 220.0
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.130 89.8
BN (mp-984) <1 0 0> <1 0 0> 0.132 155.6
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.134 220.0
Te2W (mp-22693) <1 1 0> <1 1 0> 0.135 220.0
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.144 220.0
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.146 259.3
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.146 259.3
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.147 269.5
PbS (mp-21276) <1 1 1> <1 0 0> 0.154 311.2
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.159 259.3
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.161 155.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
80 53 53 0 0 0
53 80 53 0 0 0
53 53 80 0 0 0
0 0 0 34 0 0
0 0 0 0 34 0
0 0 0 0 0 34
Compliance Tensor Sij (10-12Pa-1)
26.4 -10.5 -10.5 0 0 0
-10.5 26.4 -10.5 0 0 0
-10.5 -10.5 26.4 0 0 0
0 0 0 29.1 0 0
0 0 0 0 29.1 0
0 0 0 0 0 29.1
Shear Modulus GV
26 GPa
Bulk Modulus KV
62 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
62 GPa
Shear Modulus GVRH
24 GPa
Bulk Modulus KVRH
62 GPa
Elastic Anisotropy
1.12
Poisson's Ratio
0.33

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -2.632 23.357 3.405 7.559
pack_evans_james -2.632 23.359 0.377 3.855
vinet -2.633 23.337 3.482 5.930
tait -2.633 23.339 0.381 6.018
birch_euler -2.632 23.351 0.428 0.884
pourier_tarantola -2.635 23.327 0.067 2.929
birch_lagrange -2.640 23.342 0.251 6.480
murnaghan -2.631 23.387 0.367 3.693
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SmBiPd2 (mp-862752) 0.0000 0.080 3
PmSnRh2 (mp-862961) 0.0000 0.000 3
HfGaRu2 (mp-865010) 0.0000 0.000 3
GaFeRh2 (mp-865170) 0.0000 0.000 3
Ca2AgSn (mp-867751) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
LiMgSbPt (mp-571584) 0.0000 0.051 4
LiMgSbPd (mp-10179) 0.0000 0.090 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
K3Sr (mp-973622) 0.0000 0.117 2
Yb3Re (mp-980049) 0.0000 0.551 2
Yb3Ru (mp-979937) 0.0000 0.153 2
ReP3 (mp-974565) 0.0000 0.826 2
Na3Pu (mp-1006151) 0.0000 0.539 2
Br (mp-673171) 0.0000 0.630 1
Ti (mp-73) 0.0000 0.112 1
I (mp-684663) 0.0000 0.446 1
Cr (mp-90) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.139 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Mg_pv Hg
Final Energy/Atom
-2.6333 eV
Corrected Energy
-10.5332 eV
Uncorrected energy = -10.5332 eV Corrected energy = -10.5332 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)