Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.360 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.050 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 255.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 262.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 225.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 47.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 285.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 190.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 204.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 102.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 47.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 119.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 255.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 87.2 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 357.2 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 214.3 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 150.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 264.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 284.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 261.6 |
YVO4 (mp-19133) | <1 0 0> | <1 1 -1> | 282.0 |
YVO4 (mp-19133) | <1 0 1> | <1 1 -1> | 282.0 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 166.7 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 214.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 190.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 238.1 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 214.3 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 119.1 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 225.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 87.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 305.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 238.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 309.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 87.2 |
GaSe (mp-1943) | <1 0 0> | <1 0 -1> | 204.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 174.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 166.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 214.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 142.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 43.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 262.0 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 262.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 305.3 |
BN (mp-984) | <1 0 1> | <1 1 1> | 225.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 130.8 |
BN (mp-984) | <1 1 1> | <0 1 0> | 238.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 102.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 47.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 153.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 213.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 130.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
190 | 53 | 50 | 0 | 2 | 0 |
53 | 253 | 76 | 0 | 15 | 0 |
50 | 76 | 259 | 0 | -11 | 0 |
0 | 0 | 0 | 16 | 0 | 34 |
2 | 15 | -11 | 0 | 46 | 0 |
0 | 0 | 0 | 34 | 0 | 39 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.7 | -0.9 | -0.9 | 0 | -0.2 | 0 |
-0.9 | 4.6 | -1.3 | 0 | -1.8 | 0 |
-0.9 | -1.3 | 4.5 | 0 | 1.5 | 0 |
0 | 0 | 0 | -70.8 | 0 | 62.2 |
-0.2 | -1.8 | 1.5 | 0 | 22.7 | 0 |
0 | 0 | 0 | 62.2 | 0 | -28.8 |
Shear Modulus GV55 GPa |
Bulk Modulus KV118 GPa |
Shear Modulus GR-94 GPa |
Bulk Modulus KR114 GPa |
Shear Modulus GVRH-20 GPa |
Bulk Modulus KVRH116 GPa |
Elastic Anisotropy-7.88 |
Poisson's Ratio0.59 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2MnO3 (mp-565799) | 0.1292 | 0.000 | 3 |
Li2TiO3 (mp-2931) | 0.1338 | 0.000 | 3 |
Li2MoO3 (mp-694855) | 0.1354 | 0.111 | 3 |
Na2US3 (mp-15886) | 0.1343 | 0.000 | 3 |
Li2MnO3 (mp-18988) | 0.1300 | 0.000 | 3 |
Li3Cu(NiO2)4 (mp-772355) | 0.1419 | 0.032 | 4 |
Li3Al2CrO6 (mp-861573) | 0.1452 | 0.016 | 4 |
Li4TiCo3O8 (mp-770897) | 0.1443 | 0.063 | 4 |
Li3Al2FeO6 (mp-770727) | 0.1238 | 0.021 | 4 |
Li4TiCrO6 (mp-769687) | 0.1425 | 0.068 | 4 |
LiTe3 (mp-27466) | 0.2818 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.3565 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.3697 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.3663 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.3331 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4803 | 0.139 | 5 |
Hg (mp-982872) | 0.5339 | 0.020 | 1 |
Sb (mp-632286) | 0.4189 | 0.059 | 1 |
Te (mp-570459) | 0.4794 | 0.044 | 1 |
Te (mp-10654) | 0.5761 | 0.047 | 1 |
Te (mp-105) | 0.4573 | 0.047 | 1 |
Explore more synthesis descriptions for materials of composition LiNiO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O |
Final Energy/Atom-4.8644 eV |
Corrected Energy-69.0789 eV
-69.0789 eV = -58.3732 eV (uncorrected energy) - 6.4920 eV (MP Advanced Correction) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)