material

Al2RuPt

ID:

mp-867125

DOI:

10.17188/1311773


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.901 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.46 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 0 0> <1 0 0> 0.000 146.8
Al (mp-134) <1 1 0> <1 1 0> 0.000 207.6
Ag (mp-124) <1 0 0> <1 0 0> 0.006 293.5
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.013 146.8
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.013 207.6
C (mp-48) <0 0 1> <1 1 1> 0.021 63.5
ZnO (mp-2133) <0 0 1> <1 1 1> 0.024 254.2
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.033 155.7
C (mp-66) <1 0 0> <1 0 0> 0.036 330.2
Ni (mp-23) <1 1 0> <1 1 0> 0.040 51.9
Ni (mp-23) <1 1 1> <1 1 1> 0.040 63.5
NaCl (mp-22862) <1 0 0> <1 0 0> 0.044 293.5
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.058 73.4
Au (mp-81) <1 0 0> <1 0 0> 0.059 293.5
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.060 103.8
Ni (mp-23) <1 0 0> <1 1 0> 0.062 259.4
KCl (mp-23193) <1 0 0> <1 0 0> 0.083 330.2
ZnO (mp-2133) <1 0 1> <1 0 0> 0.102 220.1
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.121 293.5
SiC (mp-11714) <0 0 1> <1 1 1> 0.124 254.2
SiC (mp-7631) <0 0 1> <1 1 1> 0.138 254.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.152 36.7
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.156 190.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.157 51.9
AlN (mp-661) <0 0 1> <1 0 0> 0.163 293.5
TiO2 (mp-390) <0 0 1> <1 0 0> 0.165 73.4
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.177 155.7
C (mp-66) <1 1 0> <1 1 0> 0.180 311.3
GaAs (mp-2534) <1 0 0> <1 0 0> 0.189 293.5
C (mp-48) <1 1 0> <1 0 0> 0.197 330.2
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.207 293.5
GaN (mp-804) <1 0 0> <1 0 0> 0.250 183.5
Mg (mp-153) <1 0 0> <1 0 0> 0.259 183.5
ZnO (mp-2133) <1 0 0> <1 1 1> 0.279 317.7
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.291 155.7
LaF3 (mp-905) <1 0 0> <1 1 1> 0.293 317.7
PbS (mp-21276) <1 0 0> <1 0 0> 0.312 36.7
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.315 146.8
PbS (mp-21276) <1 1 0> <1 1 0> 0.322 51.9
PbS (mp-21276) <1 1 1> <1 1 1> 0.323 63.5
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.325 311.3
Ge (mp-32) <1 0 0> <1 0 0> 0.331 293.5
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.335 146.8
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.348 183.5
Si (mp-149) <1 0 0> <1 0 0> 0.353 146.8
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.376 207.6
Cu (mp-30) <1 1 0> <1 1 0> 0.398 207.6
C (mp-48) <1 0 1> <1 0 0> 0.408 220.1
SiO2 (mp-6930) <1 0 1> <1 1 1> 0.446 317.7
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.446 220.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
309 147 147 0 0 0
147 309 147 0 0 0
147 147 309 0 0 0
0 0 0 110 0 0
0 0 0 0 110 0
0 0 0 0 0 110
Compliance Tensor Sij (10-12Pa-1)
4.7 -1.5 -1.5 0 0 0
-1.5 4.7 -1.5 0 0 0
-1.5 -1.5 4.7 0 0 0
0 0 0 9.1 0 0
0 0 0 0 9.1 0
0 0 0 0 0 9.1
Shear Modulus GV
99 GPa
Bulk Modulus KV
201 GPa
Shear Modulus GR
96 GPa
Bulk Modulus KR
201 GPa
Shear Modulus GVRH
97 GPa
Bulk Modulus KVRH
201 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ScBiPd2 (mp-973126) 0.0000 0.075 3
NbGaFe2 (mp-977410) 0.0000 0.000 3
NaLaAu2 (mp-865098) 0.0000 0.000 3
Tm2AgRu (mp-865282) 0.0000 0.000 3
Be2CuPt (mp-865869) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
LiMgSbPt (mp-571584) 0.0000 0.086 4
LiMgSbPd (mp-10179) 0.0000 0.074 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
K3Cd (mp-983062) 0.0000 0.057 2
K3Sc (mp-973535) 0.0000 0.615 2
Ag3Ge (mp-985283) 0.0000 0.100 2
Li3Zn (mp-976412) 0.0000 0.006 2
PmCd3 (mp-862899) 0.0000 0.000 2
Br (mp-673171) 0.0000 0.630 1
Ti (mp-73) 0.0000 0.112 1
I (mp-684663) 0.0000 0.446 1
Cr (mp-90) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.139 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Ru_pv Pt
Final Energy/Atom
-6.6100 eV
Corrected Energy
-26.4398 eV
-26.4398 eV = -26.4398 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation