material

TbI3

ID:

mp-867231

DOI:

10.17188/1311895


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.662 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.98 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.097 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <1 1 0> <1 0 1> 0.000 121.0
CdS (mp-672) <1 0 0> <1 1 0> 0.000 316.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.000 112.0
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.000 112.0
Al (mp-134) <1 1 1> <0 0 1> 0.001 112.0
TePb (mp-19717) <1 1 0> <1 0 0> 0.002 182.7
GaN (mp-804) <0 0 1> <1 1 0> 0.004 316.4
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.005 319.6
BN (mp-984) <1 0 1> <1 0 0> 0.006 182.7
Mg (mp-153) <1 0 0> <1 0 0> 0.007 182.7
GdScO3 (mp-5690) <0 1 0> <1 1 0> 0.007 316.4
NaCl (mp-22862) <1 1 0> <1 1 0> 0.008 316.4
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.010 137.0
LiF (mp-1138) <1 1 1> <1 0 0> 0.012 228.3
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.012 79.1
AlN (mp-661) <1 0 1> <1 0 0> 0.013 319.6
NaCl (mp-22862) <1 1 1> <1 0 0> 0.013 274.0
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.014 45.7
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.014 45.7
NaCl (mp-22862) <1 0 0> <1 1 0> 0.015 158.2
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.015 316.4
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.018 228.3
ZnO (mp-2133) <1 0 0> <1 0 0> 0.018 319.6
C (mp-66) <1 0 0> <1 1 0> 0.019 316.4
GdScO3 (mp-5690) <1 1 0> <1 1 0> 0.020 316.4
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.020 112.0
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.021 182.7
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.021 316.4
Au (mp-81) <1 0 0> <1 0 0> 0.023 319.6
Au (mp-81) <1 1 0> <1 0 0> 0.023 274.0
GaN (mp-804) <1 0 1> <1 0 0> 0.025 228.3
TbScO3 (mp-31119) <0 1 0> <1 1 0> 0.027 316.4
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.028 316.4
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.029 112.0
Al (mp-134) <1 1 0> <1 0 0> 0.031 45.7
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.032 316.4
BN (mp-984) <0 0 1> <1 0 0> 0.035 228.3
Al (mp-134) <1 0 0> <1 0 0> 0.035 182.7
CsI (mp-614603) <1 1 1> <0 0 1> 0.039 112.0
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.041 319.6
WS2 (mp-224) <0 0 1> <1 0 0> 0.043 228.3
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.044 228.3
Ag (mp-124) <1 0 0> <1 0 0> 0.048 319.6
GaN (mp-804) <1 0 0> <1 0 0> 0.048 319.6
Ag (mp-124) <1 1 0> <1 0 0> 0.051 274.0
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.053 319.6
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.057 228.3
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.057 228.3
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.063 316.4
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.066 182.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
1 1 1 0 0 0
1 1 1 0 0 0
1 1 46 0 0 0
0 0 0 0 0 0
0 0 0 0 0 0
0 0 0 0 0 0
Compliance Tensor Sij (10-12Pa-1)
1494 -1035.9 -5.6 0 0 0
-1035.9 1494 -5.6 0 0 0
-5.6 -5.6 21.8 0 0 0
0 0 0 2975.6 0 0
0 0 0 0 2975.6 0
0 0 0 0 0 5059.9
Shear Modulus GV
3 GPa
Bulk Modulus KV
6 GPa
Shear Modulus GR
0 GPa
Bulk Modulus KR
1 GPa
Shear Modulus GVRH
2 GPa
Bulk Modulus KVRH
3 GPa
Elastic Anisotropy
53.32
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
PmI3 (mp-863695) 0.0441 0.000 2
SmI3 (mp-863028) 0.0892 0.000 2
LuI3 (mp-865521) 0.0232 0.000 2
DyI3 (mp-865005) 0.0843 0.000 2
LuBr3 (mp-866214) 0.0755 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Tb_3 I
Final Energy/Atom
-3.6796 eV
Corrected Energy
-31.7104 eV
Uncorrected energy = -29.4364 eV Composition-based energy adjustment (-0.379 eV/atom x 6.0 atoms) = -2.2740 eV Corrected energy = -31.7104 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)