material

BeVFe2

ID:

mp-867304

DOI:

10.17188/1311973


Material Details

Final Magnetic Moment
0.929 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-0.232 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 1 0> <1 1 0> 0.000 343.2
GaP (mp-2490) <1 0 0> <1 0 0> 0.000 30.3
GaP (mp-2490) <1 1 0> <1 1 0> 0.000 42.9
GaP (mp-2490) <1 1 1> <1 1 1> 0.000 52.5
Ag (mp-124) <1 1 1> <1 1 1> 0.002 210.2
C (mp-48) <1 1 0> <1 1 0> 0.006 300.3
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.008 30.3
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.008 42.9
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.008 52.5
Au (mp-81) <1 1 1> <1 1 1> 0.012 210.2
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.021 128.7
Cu (mp-30) <1 1 1> <1 1 1> 0.031 157.6
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.031 210.2
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.040 42.9
WS2 (mp-224) <0 0 1> <1 0 0> 0.040 212.3
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.040 212.3
InAs (mp-20305) <1 0 0> <1 0 0> 0.049 151.7
LiF (mp-1138) <1 1 0> <1 1 0> 0.051 257.4
Mg (mp-153) <1 1 1> <1 1 0> 0.056 300.3
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.062 210.2
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.064 151.7
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.066 60.7
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.072 333.7
MoSe2 (mp-1634) <1 0 0> <1 1 0> 0.073 257.4
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.075 212.3
Mg (mp-153) <0 0 1> <1 0 0> 0.079 212.3
C (mp-48) <1 0 0> <1 1 0> 0.090 171.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.091 151.7
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.097 128.7
KCl (mp-23193) <1 1 0> <1 1 0> 0.107 171.6
KCl (mp-23193) <1 1 1> <1 1 1> 0.109 210.2
SiC (mp-8062) <1 0 0> <1 0 0> 0.112 151.7
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.118 210.2
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.119 91.0
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.156 151.7
GaN (mp-804) <1 0 0> <1 0 0> 0.160 273.0
Si (mp-149) <1 0 0> <1 0 0> 0.163 30.3
Mg (mp-153) <1 1 0> <1 1 0> 0.165 85.8
Ni (mp-23) <1 0 0> <1 0 0> 0.166 60.7
Al (mp-134) <1 1 0> <1 1 0> 0.169 257.4
Si (mp-149) <1 1 0> <1 1 0> 0.169 42.9
Si (mp-149) <1 1 1> <1 1 1> 0.171 52.5
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.172 242.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.173 30.3
ZnO (mp-2133) <1 1 1> <1 1 0> 0.179 343.2
TiO2 (mp-390) <0 0 1> <1 0 0> 0.180 242.7
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.180 42.9
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.183 52.5
CdS (mp-672) <1 0 1> <1 0 0> 0.184 364.0
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.185 212.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
340 164 164 0 0 0
164 340 164 0 0 0
164 164 340 0 0 0
0 0 0 127 0 0
0 0 0 0 127 0
0 0 0 0 0 127
Compliance Tensor Sij (10-12Pa-1)
4.3 -1.4 -1.4 0 0 0
-1.4 4.3 -1.4 0 0 0
-1.4 -1.4 4.3 0 0 0
0 0 0 7.9 0 0
0 0 0 0 7.9 0
0 0 0 0 0 7.9
Shear Modulus GV
111 GPa
Bulk Modulus KV
222 GPa
Shear Modulus GR
108 GPa
Bulk Modulus KR
222 GPa
Shear Modulus GVRH
110 GPa
Bulk Modulus KVRH
222 GPa
Elastic Anisotropy
0.16
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sc2RuAu (mp-972879) 0.0000 0.000 3
Sc2BeRu (mp-862553) 0.0000 0.039 3
LiGaRh2 (mp-862730) 0.0000 0.000 3
Y2NiRu (mp-865641) 0.0000 0.016 3
TiMn2V (mp-865678) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
LiMgSbPt (mp-571584) 0.0000 0.086 4
LiMgSbPd (mp-10179) 0.0000 0.074 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
ScCu3 (mp-973100) 0.0000 0.039 2
AlNi3 (mp-672232) 0.0000 0.047 2
Mn3Al (mp-973149) 0.0000 0.069 2
NdAu3 (mp-975073) 0.0000 0.043 2
LaCd3 (mp-862559) 0.0000 0.000 2
Br (mp-673171) 0.0000 0.630 1
Ti (mp-73) 0.0000 0.112 1
I (mp-684663) 0.0000 0.446 1
Cr (mp-90) 0.0000 0.000 1
Bi (mp-568610) 0.0000 0.139 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Be_sv V_pv Fe_pv
Final Energy/Atom
-7.6731 eV
Corrected Energy
-30.6925 eV
-30.6925 eV = -30.6925 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)