Final Magnetic Moment4.976 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.017 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.512 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63 [173] |
HallP 6c |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 1> | 107.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 106.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 185.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 215.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 264.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 246.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 246.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 213.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 88.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 264.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 264.6 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 185.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 88.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 264.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 61.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 308.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 264.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 308.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 264.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 308.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 106.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 246.6 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 185.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 308.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 185.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 308.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 308.3 |
C (mp-66) | <1 1 0> | <1 0 1> | 107.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 88.2 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 185.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 264.6 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 308.3 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 213.6 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 185.0 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 308.3 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 185.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 185.0 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 185.0 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 61.7 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 308.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 185.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 185.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 308.3 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 1> | 215.2 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 185.0 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 264.6 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 264.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La3Fe2S7 (mp-675895) | 0.4723 | 0.109 | 3 |
Na8Cu2O7 (mp-779159) | 0.5244 | 0.102 | 3 |
Na3VS4 (mp-29143) | 0.5368 | 0.000 | 3 |
Sr7GeN6 (mp-568436) | 0.5420 | 0.000 | 3 |
Na4TiSe4 (mp-505798) | 0.5235 | 0.000 | 3 |
La3MnFeS7 (mp-18484) | 0.2423 | 0.055 | 4 |
Nd3MnAlS7 (mp-864652) | 0.0858 | 0.000 | 4 |
Ce3MnAlS7 (mp-866500) | 0.1295 | 0.010 | 4 |
Ce3AlCrS7 (mp-866516) | 0.2204 | 0.004 | 4 |
Ce3MgAlS7 (mp-866517) | 0.1201 | 0.018 | 4 |
Tl4S3 (mp-2753) | 0.7341 | 0.008 | 2 |
K3WS3ClO (mp-565818) | 0.6305 | 0.168 | 5 |
Sr2AlGaNi2O7 (mvc-377) | 0.7181 | 0.160 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Mn_pv Al S |
Final Energy/Atom-6.3091 eV |
Corrected Energy-160.7079 eV
-160.7079 eV = -151.4194 eV (uncorrected energy) - 9.2884 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)