Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.595 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa2Zn17 + LaAu2 + La14Au51 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 253.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 253.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 143.3 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 286.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 263.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 215.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 253.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 253.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 202.7 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 263.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 215.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 215.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 263.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 253.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 253.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 253.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 71.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 202.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 215.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 87.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 202.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 286.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 215.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 202.7 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 253.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 71.7 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 87.8 |
BN (mp-984) | <0 0 1> | <1 1 1> | 87.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 143.3 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 286.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 152.0 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 143.3 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 87.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 286.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 215.0 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 215.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 50.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 152.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 304.0 |
Al (mp-134) | <1 1 1> | <1 0 0> | 253.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 253.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 215.0 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 87.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 152.0 |
BN (mp-984) | <1 1 0> | <1 1 1> | 263.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 286.6 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 215.0 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 286.6 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 286.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 253.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
DyYHg2 (mp-971799) | 0.0000 | 0.007 | 3 |
Si2HgTe (mp-631331) | 0.0000 | 0.720 | 3 |
NpSnRh2 (mp-864834) | 0.0000 | 0.127 | 3 |
TmCdPd2 (mp-865982) | 0.0000 | 0.000 | 3 |
ErSnRu2 (mp-866285) | 0.0000 | 0.000 | 3 |
TiFeCoAs (mp-998974) | 0.0000 | 0.134 | 4 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnGaFeCo (mp-999552) | 0.0000 | 0.044 | 4 |
CeHg (mp-702) | 0.0000 | 0.000 | 2 |
TmCu (mp-985) | 0.0000 | 0.000 | 2 |
SrCd (mp-30496) | 0.0000 | 0.000 | 2 |
HfIr (mp-1002122) | 0.0000 | 0.042 | 2 |
DyAs (mp-1010161) | 0.0000 | 0.476 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Zn Au |
Final Energy/Atom-3.7810 eV |
Corrected Energy-15.1238 eV
-15.1238 eV = -15.1238 eV (uncorrected energy)
|