Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.036 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.113 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbAgF3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmmm [65] |
Hall-C 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 232.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 68.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 297.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 207.6 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 169.8 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 310.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 296.6 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 84.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 232.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 206.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 206.4 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 299.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 339.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 118.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 275.2 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 297.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 68.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 137.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 114.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 232.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 266.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 187.5 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 337.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 326.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 266.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 310.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 262.4 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 262.4 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 299.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 278.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 127.3 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 187.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 148.3 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 254.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 344.0 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 337.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 229.4 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 232.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 250.0 |
Bi2Te3 (mp-34202) | <1 0 0> | <0 1 0> | 137.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 178.6 |
BN (mp-984) | <1 0 0> | <1 0 0> | 207.6 |
BN (mp-984) | <1 1 0> | <0 1 0> | 68.8 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 160.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 187.5 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 1 0> | 262.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 321.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 150.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 207.6 |
Al (mp-134) | <1 1 0> | <1 0 0> | 207.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K3NO (mp-675156) | 0.7278 | 0.661 | 3 |
YReN3 (mp-998367) | 0.7052 | 0.126 | 3 |
K3ClO (mp-673798) | 0.7038 | 0.007 | 3 |
CsPbCl3 (mp-675524) | 0.7297 | 0.003 | 3 |
SrZrO3 (mp-1068742) | 0.6694 | 0.048 | 3 |
Sr2ZnReO6 (mp-548691) | 0.7292 | 0.043 | 4 |
Sr2ReNiO6 (mp-32307) | 0.7180 | 0.190 | 4 |
MgPb2WO6 (mp-25799) | 0.6766 | 0.000 | 4 |
Sr2CoReO6 (mp-561753) | 0.7162 | 0.030 | 4 |
Sr2CoReO6 (mp-31515) | 0.7284 | 0.030 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Ag F |
Final Energy/Atom-3.6511 eV |
Corrected Energy-18.2556 eV
-18.2556 eV = -18.2556 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)