Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.264 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 281.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 292.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 238.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 281.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 159.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 238.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 318.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 159.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 238.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 168.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 281.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 281.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 281.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 238.9 |
BN (mp-984) | <1 1 0> | <1 0 0> | 225.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 281.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 292.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 292.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 318.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 281.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 238.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 225.2 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 238.9 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 292.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 281.5 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 281.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 281.5 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 281.5 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 318.5 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 292.6 |
C (mp-66) | <1 1 1> | <1 1 1> | 292.6 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 159.3 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 159.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 281.5 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 281.5 |
InP (mp-20351) | <1 1 1> | <1 1 0> | 318.5 |
Ni (mp-23) | <1 1 1> | <1 1 0> | 318.5 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 238.9 |
InSb (mp-20012) | <1 1 1> | <1 1 1> | 292.6 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 159.3 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 281.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 281.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 168.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 168.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 292.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 281.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 159.3 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 318.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 159.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 225.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
71 | 40 | 40 | 0 | 0 | 0 |
40 | 71 | 40 | 0 | 0 | 0 |
40 | 40 | 71 | 0 | 0 | 0 |
0 | 0 | 0 | 48 | 0 | 0 |
0 | 0 | 0 | 0 | 48 | 0 |
0 | 0 | 0 | 0 | 0 | 48 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
24.1 | -8.7 | -8.7 | 0 | 0 | 0 |
-8.7 | 24.1 | -8.7 | 0 | 0 | 0 |
-8.7 | -8.7 | 24.1 | 0 | 0 | 0 |
0 | 0 | 0 | 20.6 | 0 | 0 |
0 | 0 | 0 | 0 | 20.6 | 0 |
0 | 0 | 0 | 0 | 0 | 20.6 |
Shear Modulus GV35 GPa |
Bulk Modulus KV50 GPa |
Shear Modulus GR26 GPa |
Bulk Modulus KR50 GPa |
Shear Modulus GVRH31 GPa |
Bulk Modulus KVRH50 GPa |
Elastic Anisotropy1.80 |
Poisson's Ratio0.25 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YErTl2 (mp-981548) | 0.0000 | 0.000 | 3 |
TbAlAg2 (mp-977394) | 0.0000 | 0.006 | 3 |
NdLuMg2 (mp-975515) | 0.0000 | 0.009 | 3 |
Li2AcTl (mp-976333) | 0.0000 | 0.000 | 3 |
NaCeAu2 (mp-865080) | 0.0000 | 0.017 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.163 | 4 |
Sn3B (mp-978917) | 0.0000 | 0.937 | 2 |
MgSn3 (mp-1094230) | 0.0000 | 0.091 | 2 |
Rb3Nd (mp-974850) | 0.0000 | 0.613 | 2 |
Ti3Si (mp-998986) | 0.0000 | 0.194 | 2 |
LiB (mp-1001831) | 0.0000 | 0.386 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Mg_pv Al |
Final Energy/Atom-3.9595 eV |
Corrected Energy-15.8382 eV
-15.8382 eV = -15.8382 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)