Final Magnetic Moment19.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.552 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnCr2O4 + LiNbO3 + LiMnNbO4 + Li3NbO4 |
Band Gap0.107 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 308.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 61.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 323.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 268.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 185.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 268.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 258.6 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 268.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 244.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 246.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 258.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 211.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 323.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 308.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 323.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 323.2 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 185.2 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 185.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 258.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 323.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 211.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 308.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 308.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 246.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 193.9 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 105.8 |
Al (mp-134) | <1 0 0> | <1 1 0> | 244.9 |
Al (mp-134) | <1 1 0> | <0 1 0> | 211.5 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 185.2 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 185.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 193.9 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 129.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 185.2 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 129.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 64.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 308.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 258.6 |
C (mp-66) | <1 0 0> | <1 0 0> | 308.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 308.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 185.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 323.2 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 129.3 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 323.2 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 185.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 258.6 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 61.7 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 185.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 323.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe3O8 (mp-771620) | 0.2893 | 0.104 | 3 |
Li3Mn3O8 (mp-771745) | 0.2757 | 0.076 | 3 |
Ca(MoO2)2 (mvc-10002) | 0.2892 | 0.130 | 3 |
Ca(WO2)2 (mvc-10243) | 0.3048 | 0.329 | 3 |
Ca(WO2)2 (mvc-10486) | 0.2507 | 0.384 | 3 |
Li6V3Sb3O16 (mp-775699) | 0.2235 | 0.067 | 4 |
Li6Fe3Sb3O16 (mp-771508) | 0.2019 | 0.073 | 4 |
Li4Mn5Nb3O16 (mp-773388) | 0.2161 | 0.083 | 4 |
Li6Cr3Sb3O16 (mp-773191) | 0.2210 | 0.079 | 4 |
Li4Mn5Sb3O16 (mp-769848) | 0.1897 | 0.038 | 4 |
Si3N4 (mp-641539) | 0.4844 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4367 | 0.208 | 2 |
Fe3O4 (mp-542433) | 0.5232 | 0.072 | 2 |
Fe3O4 (mp-650112) | 0.5130 | 0.057 | 2 |
Fe3O4 (mp-715811) | 0.5266 | 0.076 | 2 |
Li4Mn2Cr3Sb3O16 (mp-767785) | 0.0641 | 0.045 | 5 |
Li4Cr3Fe2Sb3O16 (mp-773763) | 0.1218 | 0.597 | 5 |
Li4V3Fe2Sb3O16 (mp-853181) | 0.1162 | 0.039 | 5 |
Li4Mn2V3Sb3O16 (mp-765741) | 0.0810 | 0.031 | 5 |
Li4Fe3Co2Sb3O16 (mp-776141) | 0.1072 | 0.094 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Nb_pv Cr_pv O |
Final Energy/Atom-7.6857 eV |
Corrected Energy-235.8364 eV
-235.8364 eV = -215.1991 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 9.4007 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)