Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.574 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4 |
Band Gap3.381 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 120.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 205.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 260.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 32.5 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 288.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 325.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 162.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 260.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 227.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 181.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 227.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 230.9 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 230.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 120.8 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 68.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 195.1 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 274.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 173.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 120.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 307.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 205.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 230.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 143.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 143.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 325.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 227.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 333.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 260.1 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 230.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 230.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 230.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 230.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 230.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 260.1 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 230.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 260.1 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 205.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 260.1 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 288.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 357.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 260.1 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 230.9 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 302.1 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 173.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 173.2 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 97.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 137.2 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 65.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 130.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 60.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAg2F4 (mp-752878) | 0.3891 | 0.047 | 3 |
V3BO6 (mp-770370) | 0.5200 | 0.109 | 3 |
Cr(AgO2)2 (mp-557056) | 0.2030 | 0.023 | 3 |
Cr3BO6 (mp-24912) | 0.5253 | 0.183 | 3 |
Mn(AgO2)2 (mp-554049) | 0.2398 | 0.185 | 3 |
MnVAgO4 (mp-558718) | 0.3952 | 0.023 | 4 |
LiFePO4 (mp-850917) | 0.2582 | 0.379 | 4 |
LiMnSiO4 (mp-780533) | 0.3673 | 0.044 | 4 |
LiCrPO4 (mp-761397) | 0.3169 | 0.075 | 4 |
LiNiPO4 (mp-762173) | 0.3274 | 0.189 | 4 |
Li7Mn7P6(O8F)3 (mp-763896) | 0.6040 | 0.022 | 5 |
Li7V7P6(O8F)3 (mp-763895) | 0.6088 | 0.131 | 5 |
Li4V2Si(PO6)2 (mp-770404) | 0.5823 | 0.077 | 5 |
Li4Nb2Fe3Te3O16 (mp-765556) | 0.5940 | 0.259 | 5 |
Na2TiZn2SiO7 (mp-13810) | 0.5829 | 0.000 | 5 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.5973 | 0.008 | 6 |
Explore more synthesis descriptions for materials of composition LiMnPO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.1152 eV |
Corrected Energy-217.1844 eV
-217.1844 eV = -199.2243 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)