Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.533 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.091 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 |
Band Gap1.712 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 170.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 170.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 170.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 260.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 130.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 130.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 130.4 |
Au (mp-81) | <1 0 0> | <1 0 0> | 260.8 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 260.8 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 260.8 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 170.5 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 260.8 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 130.4 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 130.4 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 170.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2SiO4 (mp-3789) | 0.3187 | 0.000 | 3 |
Be(GaO2)2 (mp-757917) | 0.3142 | 0.000 | 3 |
Li2BeF4 (mp-4622) | 0.3167 | 0.000 | 3 |
Li2SeO4 (mp-4855) | 0.3313 | 0.000 | 3 |
Li2MoO4 (mp-25080) | 0.3283 | 0.000 | 3 |
LiFeSiO4 (mp-863887) | 0.2584 | 0.352 | 4 |
LiVSiO4 (mp-767474) | 0.2617 | 0.149 | 4 |
LiFeSiO4 (mp-763625) | 0.2209 | 0.059 | 4 |
LiCoSiO4 (mp-763563) | 0.2232 | 0.068 | 4 |
LiFeSiO4 (mp-762678) | 0.2668 | 0.006 | 4 |
BN (mp-1077506) | 0.5345 | 0.302 | 2 |
Si3N4 (mp-988) | 0.5453 | 0.000 | 2 |
SiC2 (mp-1019097) | 0.4899 | 0.562 | 2 |
CN2 (mp-1077595) | 0.4478 | 0.691 | 2 |
Ge3N4 (mp-13852) | 0.5215 | 0.002 | 2 |
Be3Fe4Si3SO12 (mp-627398) | 0.5193 | 0.000 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.4816 | 0.000 | 5 |
Li4Al3Ge3IO12 (mp-557456) | 0.5068 | 0.000 | 5 |
Li4Ga3Si3BrO12 (mp-556649) | 0.5109 | 0.000 | 5 |
Mn4Be3Ge3SeO12 (mp-25766) | 0.5284 | 0.000 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.5443 | 0.003 | 6 |
C (mp-680372) | 0.7235 | 0.407 | 1 |
C (mp-568410) | 0.4708 | 0.507 | 1 |
C (mp-1008374) | 0.4874 | 0.437 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-6.8279 eV |
Corrected Energy-320.0248 eV
-320.0248 eV = -286.7718 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 16.3980 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)